Eldon,
The first thing I would do is check to see if the W/S fixtures have been damaged or replaced with new ones... Then I would ask who's the new guy in the wave solder room...
Paul
Paul Edwards
Surface Art Engineering
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Eldon Sanders
Sent: Friday, July 02, 2010 4:31 PM
To: [log in to unmask]
Subject: [TN] Cracked 2208 smt resistor end joint - Found word(s) list error in the Text body
We are experiencing fractures in the end metallization or solder joint on one of
two larger high voltage resistors, size 2208. They are mounted on FR-4.
Only one location is failing. The other location is an inch away and oriented at
90 degrees. The failure rate is variable between assembly lots. Some have
no failures, and no observed cracks. The most recent lot has a 2% failure
rate, and another 2% that exhibit visible cracks in the ceramic but the solder
joint is connecting the pad to the metallization and making electrical
connection. I believe the root cause is the poor choice of the FR-4 board
material with such a large ceramic resistor. However, about 80,000 boards
have been built over 7 years without this failure mode. So, I am searching for
the root cause of this specific timeframe. I have verified the process at the
CM has not changed - the resistor is mounted on the 2nd pass SMT, and the
board goes through wave soldering of TH components using a fixture. The
same date code resistor is used for both good assembly lots and bad. There
is some correlation to the date code of the bare fab. On cracked boards
there is a gap observable between the solder joint and the ceramic resistor
body.
My present theory is the crack occurs when the assembly is wave soldered
causing excessive tension on the resistor due to CTE mis-match, and some of
these crack. But when the board comes back to ambient it seems to be
longer, and shows a gap. After a board goes through 3 heat cycles at a CM,
wouldn't it be stable in CTE? And why would the other resistor not have the
same issue? Is CTE different in X and Y? Finally, would an error or change in
the raw fab process cause a change in the CTE and cause this issue to occur
after many years?
Thanks to all the incredible minds if TechNet.
Eldon Sanders
Sr. Manufacturing Engineer
Welch Allyn Monitoring
8500 SW Creekside Place
Beaverton, OR 97008-7107
phone: (503) 530-7596 fax: (503) 526-4300
[log in to unmask]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
==============================================================================
This email and any attachments thereto may contain private, confidential, and
privileged material for the sole use of the intended recipient. Any review, copying,
or distribution of this email (or any attachments thereto) by others is strictly prohibited.
If you are not the intended recipient, please contact [log in to unmask]
immediately and permanently delete the original and any copies of this email and
any attachments thereto.
==============================================================================
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|