TECHNET Archives

July 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Werner Engelmaier <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Werner Engelmaier <[log in to unmask]>
Date:
Tue, 20 Jul 2010 11:19:19 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (158 lines)
 Hi Dale,
Do you mean CGA's [column grid arrays]? If not, what do you mean by cca?

 610, Class 3 or otherwise, only addresses quality, not reliability—for that you need to go to IPC-D-279.

While the absence of solder fillets can reduce fatigue life, the presence of fillets, 'robust' or otherwise, does not have any positive first-order impact. However, solder joint height does.


 You may be looking at IMC crystals.
Werner

 

-----Original Message-----
From: Hart, Dale L CTR USAF AFMC AFRL/RXSA <[log in to unmask]>
To: [log in to unmask]
Sent: Tue, Jul 20, 2010 9:23 am
Subject: [TN] solder joint height


 



We have been doing a some analysis of cca's for the Air Force consisting of

SMT.  The visual inspection of the solder joints looks very good all

characteristics above the suggest minimum for class 3 of 610.  The solder

fillets in some instances could be characterized as being robust.  In

cross-sectional analysis however, the solder joint height of the components

electrical termination above the land has been perhaps 0.025 mm to the point

of needing a SEM to look at the land-solder-component lead interface.

Closer examination in these areas revealed small cracks in the grain

boundaries.  I used the term grain boundaries because the solder in these

areas do not resemble the colonies observed in the bulk solder of the

fillet.  In some of these instances the land is often deformed in the shape

of the component lead.  



 



Would these joints although stronger be more susceptible to fatigue or

overload failure?



What are the implications if these cca's are encapsulated?



What suggestions could be offered to the manufacturer?



 



 



Dale L. Hart



Universal Technology Corporation (UTC)



Failure Analysis



1270 North Fairfield Road



Dayton, Ohio  45432-2600



(937) 656-9165



Fax (937) 656-4600



Email:  <mailto:[log in to unmask]> [log in to unmask]



 





---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to 

[log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to 

[log in to unmask]: SET Technet Digest

Search the archives of previous posts at: http://listserv.ipc.org/archives

Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for 

additional information, or contact Keach Sasamori at [log in to unmask] or 

847-615-7100 ext.2815

-----------------------------------------------------


 

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2