TECHNET Archives

July 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Paul Reid <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Paul Reid <[log in to unmask]>
Date:
Thu, 15 Jul 2010 17:33:23 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (405 lines)
Yes, I think yours is a correct overview of what I am trying to express.

I do not think that air filled voids exert significant pressure at 260°C. 

PR

Hi,

 A Question:

  I would think, and I might be wrong, that once water is in a vapor form it
would pretty much follows the ideal gas law. So, would water vapor in a PCB
structure behave much like air or any other gas? Is that correct? 

 Would an air filled section of a PCB generate pressures equivalent to water
filled areas?

Bob Kondner

 



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Paul Edwards
Sent: Thursday, July 15, 2010 3:22 PM
To: [log in to unmask]
Subject: Re: [TN] BAKING OF PWB QUESTION

I'm with Werner on this...

I am concerned with the general statements made that:

"Basically we are saying that many studies demonstrate limited impact,
positive or negative, on reliability due to baking. Dr. Taube shows
"moisture in" or "moisture out" has a limited reliability affect. The effect
of baking is not compelling for extending ability to survive assembly and
rework."

I can tell you that numerous assemblies and reworks have been done
successfully due to the pre-baking of components, PCBs and assemblies...

We have run both no bake and pre-baked processes and found consistently that
the pre-baked materials always yields higher finished product...

If baking out moisture did not increase reliability then there would be no
detrimental effect to the unlimited exposure of non-ceramic BGAs to
moisture...After all most BGAs use a PCB-like substrate...

Paul

Paul Edwards
Surface Art Engineering


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier
Sent: Thursday, July 15, 2010 12:01 PM
To: [log in to unmask]
Subject: Re: [TN] BAKING OF PWB QUESTION

 Hi Paul,
I think we went over the water vapor/steam issue once before.
It simply is not so that one needs liquid water to have an increase in
pressure.
Consider a closed vessel with some water in it. As you heat the vessel the
liquid water will vaporize until all of it has vaporized. Just because you
no longer have liquid H2O does not mean that the pressure does not increase
with increasing T-you now have superheated steam that follows the equation
P= RT/V-so the higher the temperature the higher the pressure for a constant
volume. V certainly can increase with delamination and some of the
superheated steam will escape. The term 'live steam' has no meaning in this
context-its primary use is for model railroading, and refers to steam
actually doing some work in driving the locomotive. Inside the PCB, liquid
water per se does hardly ever exist, the steam does do 'work' only in terms
of increasing the internal vapor pressure, and you certainly do not need
liquid water for that.
Werner

 


 

 

-----Original Message-----
From: Paul Reid <[log in to unmask]>
To: [log in to unmask]
Sent: Thu, Jul 15, 2010 11:37 am
Subject: Re: [TN] BAKING OF PWB QUESTION


This is a good thread. 



Off-line Ian Hanna from Circuit Tech comments:  



"Hey Paul,  I would expect that the biggest threat from trapped moisture is
the 

vapour pressures generated during the initial shock of assembly...would this
be 

visible during cyclic reliability testing?  Regards - Ian"



The answer to Ian's question is, yes, the greatest "threat" (or at least 

pressure) from trapped moisture is during the initial thermal excursion and
yes 

it is visible during reliability testing. But no we do not see delamination 

during the first thermal cycle and if the material delaminates the effect is


extended cycles to failure. The lesson is you have to test both the copper
and 

the material when doing reliability testing for lead/free applications
incase 

the material degrades and you get false positives from thermal cycle
testing. We 

measure material damage by means of changes in capacitance in representative


coupons in order to capture material damage.



Basically we are saying that many studies demonstrate limited impact,
positive 

or negative, on reliability due to baking. Dr. Taube shows "moisture in" or 

"moisture out" has a limited reliability affect. The effect of baking is not


compelling for extending ability to survive assembly and rework.



The idea is that vapor pressure from trapped water "blows" the material
apart. 

It is my contention that if the adhesion between laminated surfaces is weak,
by 

that I mean, between B-stage and C-stage or B-stage and copper, then vapor 

pressure generated from trapped water may cause frank delamination. But
there is 

more to this story.



I expect the greatest pressure from water vapor would occur during heating
on 

the first thermal excursion because the board has the greatest amount of
water 

at the beginning of assembly. After the first cycle moisture must have been
out 

gassing during the thermal excursion. The longer at temperature the less
water 

in the board so by the second thermal excursion there should be less
pressure 

because some of the water has been lost. Our findings are consistent with
Dr. 

Taube's findings. Delamination does not typically occur on the first thermal


cycle. Delamination frequently occurs after the third thermal excursion.
Let's 

let that stand for a second.



Dr. Wayne Rothschild points out that the vapor pressure is limited by the
amount 

of water available to the system. He points out that the gas laws take into 

account the amount of water in the system.



Pressure increases rapidly with "live steam" but, when the water is all 

vaporized, the pressure increase is reduced. "Live steam" requires liquid
water 

as a source to replace the steam. A steam train stops when it runs out of
water. 

The vapor pressure goes to zero once the water escapes out of the board. 



So bringing Dr. Taube's and Dr. Rothschild's observations, our experience in


reliability testing, and how samples fail in T260 testing on a TMA,
together, I 

feel that the damage to material is from vapor pressure, z-axis expansion
and 

also material degradation. The epoxy system is failing and volatiles are 

providing a force as is z-axis expansion of the epoxy system, to a point
were 

force is greater than the strength of the epoxy and the board fails. Epoxy 

degradation is a major component of the failures and aggressive baking could


degrade the epoxy reducing reliability in a lead/free application.



All this stands given that the copper is not being degraded by 260°C, which
I, 

and others are beginning expect it is changing, when the copper is poorly
plated 

and of a lower quality. But that is another story. 







Sincerely, 

Paul Reid 



Program Coordinator 

PWB Interconnect Solutions Inc. 

235 Stafford Rd., West, Unit 103 

Nepean, Ontario 

Canada, K2H 9C1 

613 596 4244 ext. 229 

Skype paul_reid_pwb 

[log in to unmask] <mailto:[log in to unmask]> 





______________________________________________________________________

This email has been scanned by the MessageLabs Email Security System.

For more information please contact helpdesk at x2960 or [log in to unmask] 

______________________________________________________________________



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to 

[log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to 

[log in to unmask]: SET Technet Digest

Search the archives of previous posts at: http://listserv.ipc.org/archives

Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for 

additional information, or contact Keach Sasamori at [log in to unmask] or 

847-615-7100 ext.2815

-----------------------------------------------------


 

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


============================================================================
==

This email and any attachments thereto may contain private, confidential,
and
privileged material for the sole use of the intended recipient. Any review,
copying,
or distribution of this email (or any attachments thereto) by others is
strictly prohibited.
If you are not the intended recipient, please contact
[log in to unmask]
immediately and permanently delete the original and any copies of this email
and
any attachments thereto. 

============================================================================
==


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2