Hi Bob - my vote would be to reball the device using a service provider
that can demonstrate a qualified reballing process.
Dave Hillman
Rockwell Collins
[log in to unmask]
Bob Landman <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
07/09/2010 09:05 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Bob Landman <[log in to unmask]>
To
[log in to unmask]
cc
Subject
[TN] Interposer for SAC BGA
I have to use a new FPGA from Lattice and they are not offering it in
SnPb, only SAC balls. This is a fpBGA 23mm sq with 484 balls in a square
array with no special heatsink pads.
Environment is -40 to +85C, mild vibration and shock, outside environment
in electrical NEMA enclosures.
SnPb is a must - I refuse to use lead free process for our products.
Two choices:
Interposer board (Bill Rollins just told me about this option
Reballing
Comments please on your preference.
Bob Landman
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------