Hi,
I need you help,appreciate you if you can give some useful suggestion
Now a product that called Mini SAS is making in my compay,it is a cable
assembly, consist by two PCB ,36 way wires,heat shrink
tubing,innermold,overmold,etc.The wire diagram is one to one,two ends are
36PIN PCB.
The PCB is 36 PIN(18PIN in each surface) and the pitch between each pad are
very small, PCB pad width is 0.6mm and the pitch is 0.8mm,the operator weld
the conduct of wires to PCB pad by HOT-BAR(auto welding maching),
the key problem is after welding and testing there have many badness goods
be made,like as short,open,insulation resistance is very small between each
pin(<1M Ohm),just low than 70% goods could be passed test.
Pls give your prefessional advice how to solve this problem,for instance
PCB designing improve?
Sn component imrpove?
Welding machine parameter?
http://www.google.com.hk/images?hl=zh-CN&q=MINI%20SAS%20PCB&um=1&ie=UTF-8&so
urce=og&sa=N&tab=wi
(This web link to MINI SAS 36PIN products,FYI)
Thank you!
Tony Liu
Sales Department
Mobile:13048936174
18926869763
Tel£º 0769-22810730
Fax£º0769-22810732
Email:[log in to unmask]
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|