Hi Bill,
Indeed, larger footprints are a recipe for not only tombstoning, but component cracking as well.
Werner
-----Original Message-----
From: Brooks, Bill <[log in to unmask]>
To: [log in to unmask]
Sent: Wed, Jul 7, 2010 2:37 pm
Subject: [TN] 0201 footprint requirements
I am looking for some assistance with the pad geometries for 0201 caps
and resistors...
Is there or is there not an industry consensus on what the optimum pad
geometry should be for them?
What I am hearing from our assembly houses differs greatly from what is
published in IPC-7351 and the land pattern tool from PCB Matrix.
Is the max material condition footprint actually a recipe for
tombstoning?
What have you folks seen? What do you recommend?
Bill Brooks | Datron World Communications, Inc.
PCB Designer/Engineer | Office: 760-602-7004| Fax: 760-597-3777 |
[log in to unmask]
1808 Aston Avenue, Suite 230, Carlsbad, CA 92008 | www.dtwc.com
Performance You Require. Value You ExpectTM
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|