TECHNET Archives

July 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Kenneth Wood <[log in to unmask]>, TechNet E-Mail Forum <[log in to unmask]>
Date:
Wed, 28 Jul 2010 10:00:27 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Syed Ahmad <[log in to unmask]>
Subject:
From:
Syed Ahmad <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
<002101cb2e4c$f97026a0$ec5073e0$@com>
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (161 lines)
One would need to look at many other factors such as cost, availability,
processability, CTE, Modulus, dielectric properties, manufacturability at
the subcontractor, long term use environment reliability, etc.

-----Original Message-----
From: Kenneth Wood [mailto:[log in to unmask]]
Sent: Wednesday, July 28, 2010 7:04 AM
To: 'TechNet E-Mail Forum'; 'Syed Ahmad'
Subject: RE: [TN] Non-Hygroscopic" flex circuit material

So if I read this correctly, Polypropylene is the best material to use for
low moisture absorption?
Thanks for the info too :)
Ken
_____________________________________
Kenneth J. Wood
Saturn PCB Design, Inc.
www.saturnpcb.com

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Syed Ahmad
Sent: Tuesday, July 27, 2010 1:05 PM
To: [log in to unmask]
Subject: Re: [TN] Non-Hygroscopic" flex circuit material

Moisture absorption wt %
Most of the data is from Electronic pkgg materials and their properties by
Pecht et al.

Acrylic 6
Epoxy 4
Polyimide/polyamide 3
Kevlar-49 0.5-2, 1.1
Polyester <0.8, 2PPA 1.8
Polyvinyl Chloride <0.5
Polycarbonate <0.35
BCB 0.25
Polysulfone <0.22
FR4 0.1
Parylene <0.1
Fluoropolymers 0.1
Cyanate ester 0.08
BT 0.05
Polyvinyl fluoride <0.05
LCP 0.02, 0.04
TFE/FEP/polyethylene <0.01
Polypropylene <0.005

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dan Skweres
Sent: Monday, July 26, 2010 2:25 PM
To: [log in to unmask]
Subject: Re: [TN] Non-Hygroscopic" flex circuit material

Ken,
A material that doesn't absorb moisture from the environment. Kapton is out.

:)
Dan S.
----- Original Message -----
From: "Kenneth Wood" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Monday, July 26, 2010 3:01 PM
Subject: [TN] Non-Hygroscopic" flex circuit material


Hi all.
What would you consider a "Non-Hygroscopic" flex circuit material to be?
Thanks
Ken

_____________________________________
Kenneth J. Wood
Saturn PCB Design, Inc.
www.saturnpcb.com









______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------



______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------



______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2