Per 4103 SPEC.
IPC-4101B/98 L980141 SH/SH C
L =Material Designator
98= Specification Sheet Number
0141= Nominal Laminate Thickness
SH/SH = Metal Cladding Type and Nominal Weight/ Thickness
(S refer to Copper, reverse treated electrodeposited, high temperature elongation (IPC-4562, grade 3); H means half oz copper weight )
C = Thickness Tolerance Class C
IPC-4101B/98 E2116 TW RE00
98= Specification Sheet Number
E2116= Reinforcement Style , E calss glass, 2116 reinforcement type
TW = Treated Weight Total
RE = Flow Parameter define as "Rheological Flow"
00 ¨C None Specified
you can find it from ipc-4101 spec.
Best regards!
Jan chen
> Date: Fri, 23 Jul 2010 10:38:29 -0400
> From: [log in to unmask]
> Subject: [TN] Laminate and prepreg question
> To: [log in to unmask]
>
> Hello,
>
> I would like to get some clarification on a particular laminate callout
> if someone could help..
>
>
>
> IPC-4101B/98 L980141 SH/SH C
>
>
>
> My question is, what does "L980141" refer to? I understand that L =
> Laminate, I assume 98= the specific cut sheet, 0141=?
>
>
>
> Secondly, I have a prepreg callout I am trying to decifer..
>
>
>
> IPC-4101B/98 E2116 TW RE00
>
>
>
> I think "E2116" refers to the specific reinforcement style, not sure
> what "TW" refers to, and is "RE00" referring to group B flow test type?
>
> Thanks,
>
> Dave Connitt
>
>
>
> Dave Connitt CID+
>
> Printed Circuit Designer III
>
>
>
> A Wholly Owned Subsidiary of:
>
> L3 Communications
>
> 3975 McMann Road
>
> Cincinnati, Ohio 45245
>
> Ph. 513- 943-2010 Fax 513-943-2288
>
>
>
>
>
>
>
>
>
>
>
> Confidentiality Notice
> The information transmitted, including any attached data is intended
> only for the recipient to which it is addressed and may contain
> confidential material. Any unauthorized disclosure, copying,
> distribution or reliance on the contents of this information is strictly
> prohibited and may constitute a violation of law. If you are not the
> intended recipient, please notify the sender immediately by responding
> to this e-mail and delete the message from all receiving systems.
>
> Destination Control Statement - (ITAR) Domestic
> These articles or technical data are controlled by the International
> Traffic in Arms Regulations (ITAR). They are subject to the export
> control laws of the U.S. Government. They are not to be placed in the
> public domain, exported from the U.S., or given to any foreign person in
> the U.S without the prior, specific written authorization.
>
>
>
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
_________________________________________________________________
Hotmail: Powerful Free email with security by Microsoft.
https://signup.live.com/signup.aspx?id=60969
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|