TECHNET Archives

July 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, David R1 Nelson <[log in to unmask]>
Date:
Wed, 7 Jul 2010 16:17:19 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
From:
"David D. Hillman" <[log in to unmask]>
X-cc:
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (80 lines)
Hi Dave - I recommend that you have a second sample analyzed. Nickel has
an extremely slow diffusion rate at 250C in tin/lead solder so unless you
have been "suddenly" running a large volume of ENIG pwbs or some other
source of nickel across the solder pot, you should not see such a large
jump in the Ni%. Solder can get "gritty" as nickel contamination levels of
0.25% (per AWS Soldering Handbook). I have a reference paper from either
Mackay or Thwaites in the files - I'll pull it up and let you know what
they found in their testing.

Dave Hillman
Rockwell Collins
[log in to unmask]




David R1 Nelson <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
07/07/2010 02:58 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
David R1 Nelson <[log in to unmask]>


To
[log in to unmask]
cc

Subject
[TN] Ni in Eutectic SnPb solder






We have come upon a situation where the trace element Ni is above the
J-STD-001D threshold for an assembly wave solder machine with a reading of

0.015% to 0.020%. I'd like to know if anyone has experience or knows of
any studies done to determine the impact of this higher limit on the
products produced using this equipment. All advice/references would be
appreciated.

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------



______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2