EDS wouldn't be able to pick it up. ICP was the right tool
Vladimir
SENTEC Testing Laboratory Inc.
11 Canadian Road, Unit 7.
Scarborough, ON M1R 5G1
Tel: (416) 899-1882
Fax: (905) 882-8812
www.sentec.ca
-----Original Message-----
From: David R1 Nelson <[log in to unmask]>
Sender: TechNet <[log in to unmask]>
Date: Wed, 7 Jul 2010 15:33:40
To: <[log in to unmask]>
Reply-To: TechNet E-Mail Forum <[log in to unmask]>,
David R1 Nelson <[log in to unmask]>
Subject: Re: [TN] Ni in Eutectic SnPb solder
Does ICP sound familiar. We aren't questioning the measurement technique.
Samples from other equipment were tested at the same time with no
anomalies noted. Repeated testing of the questionable equipment were also
consistent.
From:
Victor Hernandez <[log in to unmask]>
To:
[log in to unmask]
Date:
07/07/2010 03:26 PM
Subject:
Re: [TN] Ni in Eutectic SnPb solder
Sent by:
TechNet <[log in to unmask]>
How was this measurement conducted? XRF or SEM/EDX.
"X"
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David R1 Nelson
Sent: Wednesday, July 07, 2010 2:59 PM
To: [log in to unmask]
Subject: [TN] Ni in Eutectic SnPb solder
We have come upon a situation where the trace element Ni is above the
J-STD-001D threshold for an assembly wave solder machine with a reading of
0.015% to 0.020%. I'd like to know if anyone has experience or knows of
any studies done to determine the impact of this higher limit on the
products produced using this equipment. All advice/references would be
appreciated.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|