TECHNET Archives

July 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Steven Creswick <[log in to unmask]>
Date:
Fri, 30 Jul 2010 09:51:44 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
From:
Douglas Pauls <[log in to unmask]>
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (137 lines)
Thank you Steve. 
Does your silicone rule refer to cured or uncured silicone or both?  And 
when you talk about "high energy", what wattage level are we talking 
about?  How long an oxygen cycle do you recommend for burn off.

I will have to play a little with hydrogen.

Not sure if I know what you mean by arc plasma.  In in-line ones that I 
have seen are largely made for things like bare boards, and not 
assemblies.

Doug Pauls



Steven Creswick <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
07/30/2010 09:22 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Steven Creswick <[log in to unmask]>


To
[log in to unmask]
cc

Subject
Re: [TN] Plasma Chamber Maintenance






Doug,

One of our rules was - thou shalt not put silicones in the chamber!

Other than that, periodically we would use a really fine scotchbrite and
clean room vac to physically clean the interior of the chamber.

Then, as Joyce indicates, a nice high energy oxygen plasma to ash off any
remaining organics and argon to knock off a few more offensive molecules. 

From a wire bonding point of view, I have found argon with 4% hydrogen to
provide a slight edge on cleaning over straight argon.  Not sure if that
would apply to CC adhesion of not.

Have you tried the arc plasma cleaners/surface activators.  Can be made 
into
an in-line process much easier than the batch type plasmas.


Steve Creswick
http://www.linkedin.com/in/stevencreswick




-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas Pauls
Sent: Friday, July 30, 2010 9:01 AM
To: [log in to unmask]
Subject: [TN] Plasma Chamber Maintenance

Good morning all,

On a topic other than rhubarb, raiding my cubicle for prizes, and selling 
off my children, I have an actual technical question.

We have started to use plasma chambers as a preparation for conformal 
coating and are having some excellent results.  One of our IEs, with a 
background in the semiconductor industry, had indicated that the chambers 
can be items that are hard to maintain or high in maintenance costs.

So, for you plasma chamber users out there, what have your experiences 
been with plasma chamber maintenance?

Doug Pauls

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------



______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2