TECHNET Archives

July 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 30 Jul 2010 09:28:28 +0200
Reply-To:
Subject:
From:
Content-Transfer-Encoding:
8bit
In-Reply-To:
<ED0D39F80A8847E4B34144C8BC5B9910@stephenPC>
Content-Type:
text/plain; format=flowed; charset="ks_c_5601-1987"; reply-type=original
MIME-Version:
1.0
Parts/Attachments:
text/plain (109 lines)
As a customer, I would never accept the discolored boards, even if the 
function is allright.  Would you buy a car with matte paint? Hardly.  If you 
can give the customer ordinary guarantee, and he accepts that, it might 
work, however.
Inge

--------------------------------------------------
From: "Steve Gregory" <[log in to unmask]>
Sent: den 30 July 2010 03:34
To: <[log in to unmask]>
Subject: Re: [TN] PCB Discoloration

> Hi Linda!
>
> While discoloration in itself is not a defect, I would be a little worried 
> about these seven boards. Especially since the rest of the lot are not 
> discolored like this:
>
>
> http://stevezeva.homestead.com/PCB_Discoloration1.jpg
>
>
>
> I don't see any delamination in the photos, but it sure looks like the 
> boards got pretty toasty. I wonder if it was because the boards were 
> sitting over a preheater or hot plate too long. From the looks of the 
> components on the board, most of it was probably hand soldered (those PTH 
> caps converted to SMT couldn't have taken reflow), and I imagine that the 
> solid plane on on the backside of the board was a real heatsink. 
> Preheating the board would have helped with soldering the PEM nuts for 
> sure, but maybe the preheater was set too high. I know a Hakko IR 
> preheater can smoke a board if you're not careful (not that I've ever done 
> that, but I know a friend of a friend who did. Hehehehe).
>
>
>
> Anyways, those seven boards saw more heat than the rest of them did based 
> on the appearance in the photos. I don't think I'd buy off on them...
>
>
>
> Steve
>
>
>
>
>
>
>
> From: Linda Langley [mailto:[log in to unmask]]
> Sent: Thursday, July 29, 2010 1:42 PM
> To: Steve Gregory
> Subject: FW: PCB Discoloration
>
>
>
> Hi Steve,
>
>
>
> Here I go again asking for help from my experts! Can you please post these 
> pictures? So I don¡¯t have to bother the whole forum, would you know the 
> name of the board guru that could answer my questions?
>
>
>
> I am not sure if the discoloration is a defect, is this a form of 
> delaminating? Why would only seven boards turn this color? They are all 
> from the same lot.
>
>
>
> Any information will be greatly appreciated.
>
>
>
>
> Linda Langley CIT
>
> Training Specialist
>
> Jabil Circuit
>
> 248-292-6176
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to 
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to 
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
> for additional information, or contact Keach Sasamori at [log in to unmask] or 
> 847-615-7100 ext.2815
> -----------------------------------------------------  

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2