TECHNET Archives

June 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"David D. Hillman" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Mon, 28 Jun 2010 07:59:59 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (203 lines)
Hi Wayne - I think that you received some inaccurate information on the 
compatibility of ENEPIG. There is substantial published testing on the 
reliability of the ENEPIG surface finish and it is fairly robust. There 
can be a Pd embrittlement issue (similar to gold embrittlement phenomenon) 
if the ENEPIG surface finish isn't specified correctly and the soldering 
process is not controlled. Otherwise the ENEPIG surface finish is good for 
a wide variety of product applications.

Dave Hillman
Rockwell Collins
[log in to unmask]



"Thayer, Wayne - IIW" <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
06/28/2010 06:54 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
"Thayer, Wayne - IIW" <[log in to unmask]>


To
[log in to unmask]
cc

Subject
Re: [TN] QFP short at top of the leads






Unstable intermetallics, apparently due to Pb and Pd refusing to form any 
intermetallic compounds.  I recall the days of PdAg finishes on ceramic 
capacitors--SnPb eutectic solder had weird wetting characteristics where 
the joint would "bloat" far away from where the heat was applied.

I've also seen odd intermetallic behavior with Bi alloys.

Wayne

-----Original Message-----
From: Wenger, George M. [mailto:[log in to unmask]] 
Sent: Monday, June 28, 2010 7:34 AM
To: TechNet E-Mail Forum; Thayer, Wayne - IIW
Subject: RE: [TN] QFP short at top of the leads

Wayne,

What makes ENEPIG incompatible with SnPb solder?

Regards,
George
George M. Wenger
Andrew Solutions
Senior Principal FMA/Reliability Engineer
40 Technology Drive, Warren, NJ 07059
(908) 546-4531 (Office) (732) 309-8964 (cell)
[log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Thayer, Wayne - IIW
Sent: Monday, June 28, 2010 7:21 AM
To: [log in to unmask]
Subject: Re: [TN] QFP short at top of the leads

Need to know the metallurgy.  What is the lead plating spec, and what 
alloy are you soldering with?  Note that ENEPIG is incompatible with SnPb 
solder.

Wayne Thayer

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Rex Waygood
Sent: Monday, June 28, 2010 6:53 AM
To: [log in to unmask]
Subject: Re: [TN] QFP short at top of the leads

Are these virgin parts?
Are the leg to pad joints 'good'?
Rex

 Rex Waygood
Technical Manager

Hansatech EMS provides value manufacturing through engineering and
quality

Hansatech EMS Limited
Benson Road
Nuffield Industrial Estate
Poole
Dorset
BH17 0RY

+44 (0)1202 338200


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Iven, Jowan
Sent: 28 June 2010 10:08
To: [log in to unmask]
Subject: [TN] QFP short at top of the leads

Has anyone ever seen a QFP where shorts occur after soldering at the top
of the leads?
And the leads look pretty dull after soldering.  Any ideas?


A picture is available at
http://ipc-technet.groupsite.com/uploads/galleries/x/000/020/5ba/technet
01.jpg

Jowan Iven




______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------

This e-mail and any files transmitted with it may be proprietary and are 
intended solely for the use of the individual or entity to whom they are 
addressed. If you have received this e-mail in error please notify the 
sender.
Please note that any views or opinions presented in this e-mail are solely 
those of the author and do not necessarily represent those of ITT 
Corporation. The recipient should check this e-mail and any attachments 
for the presence of viruses. ITT accepts no liability for any damage 
caused by any virus transmitted by this e-mail.

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------



______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2