Wayne-
Thanks. Yes they all have seen severe mechanical stress. I think the one with fatigue banding is an example of my customer's HALT/HASS. The others have likely been fielded. I'm sure that the basic experiment is to correlate HALT cycles to operational hours. However, as one can see there are different modes. Duh. But, the differences can be rather difficult to detect.
As Werner said, the situation appears to be confounded by poor joint formation, but the wetting is such that the fillets look good.
All of this is outside the scope of my engagement (nod to Werner, and setup for Dewey). Just doing a little self-guided learning. Thought maybe somebody could glean from the few pictures enough to say that they had the T-shirt.
Vladimir- once I get the ring, I'll hire Werner (I've got a hotline to him), or somebody. We try to stay on the T&M side of the gig.
Again, sorry for the cryptic nature of the postings. Have to keep it anonymous.
Chris
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Thayer, Wayne - IIW
Sent: Thursday, June 17, 2010 4:34 PM
To: [log in to unmask]
Subject: Re: [TN] solder joint failures
Very pretty pictures!
These look like different failure modes--some along the interface and some in the intermetallic area and one which looks like a crack in the solder.
All three are possible with a bunch of severe mechanical stress.
Wayne
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Chris Mahanna
Sent: Thursday, June 17, 2010 12:57 PM
To: [log in to unmask]
Subject: [TN] solder joint failures
So we’ve got a new toy, and now can image SJ failures a little differently. Requesting all experts to help me speak more intelligently about what we see. (until AJ-820 is published ☺)
These are of major interest to me today. It’s the easy stuff. It’s the weak link. It’s thru hole. As always, I may or may not know the history. As an independent lab, our customers don’t usually tell us much. I suppose they’re fearful that we may just regurgitate.
http://ipc-technet.groupsite.com/gallery/13892
Chris
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
This e-mail and any files transmitted with it may be proprietary and are intended solely for the use of the individual or entity to whom they are addressed. If you have received this e-mail in error please notify the sender.
Please note that any views or opinions presented in this e-mail are solely those of the author and do not necessarily represent those of ITT Corporation. The recipient should check this e-mail and any attachments for the presence of viruses. ITT accepts no liability for any damage caused by any virus transmitted by this e-mail.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|