There are several previous threads on this forum about this subject.
We have had this process qualified for a single BGA on a single pcb with
a certain reflow profile.
That profile produced complete reflow of the ball with no interface
between the alloys, there was a new hybrid alloy ball.
NPL published a report which is still on their website which showed good
results for the conditions of their experiment.
There were certainly negative feelings from others on the forum.
Regards
Rex
Rex Waygood
Technical Manager
Hansatech EMS provides value manufacturing through engineering and
quality
Hansatech EMS Limited
Benson Road
Nuffield Industrial Estate
Poole
Dorset
BH17 0RY
+44 (0)1202 338200
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dee Stover
Sent: 10 June 2010 15:13
To: [log in to unmask]
Subject: [TN] rohs, BGAs & assembly
Hi all,
I need to find some written data on the long term reliability of rohs
assemblies. We don't have comply with rohs but can only get the parts
in rohs, with BGA's being the main drive for rohs compliant solder.
Just had an assembly vendor say that a rohs bga can be assembled with
eutectic solder paste with good results. 2 other assembly shops say
that is not recommended. Is there any real studies or data available
that provides the real answer? Also studies and data for the
reliability of rohs? We need our boxes to work for 10 years or more.
Thank you for your time. What a great network for people to share
knowledge. I will also be going through PCD&F and google to (hopelessly
behind on my reading)
:-) Dee Stover [log in to unmask] 520-318-8489
Tech Associate II
National Optical Astronomy Observatories www.noao.edu
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|