The short answer is that ROHS really hasn't been in full use for much more than 7 years, so long term real-life experience is negligible. Most examinations that I have seen with regard to ROHS has been to estimate the expected life-span. For Lead-based systems, we have well over 40-50 years of experience as an industry to draw upon.
That being said, the general recommendation from multiple seminars, vendors and past experience is make the choice of go "ROHS" or stay with Eutectic solder through the whole assembly for that CCA. Both choices will have different set of requirements that you need to pay attention to with regards to board material, part selection, part modification/re-ball.
The primary concern with either process is most often of the BGAs, and your general choice here is go 100% lead-free or re-ball the bga. The cost is generally not prohibitive in low quantities, which I'm assuming this is. Many of the other "ROHS" parts will have a finish (bright tin/matte tin, gold, etc) that is generally compatible with either process.
Take care and hopefully I didn't open too many cans of worms:)
-Jeffrey
Jeffrey A. Jenkins CID+/CIT
Sr. PCB/CAD Designer
L-3 Communications - Linkabit Division - San Diego
Office: 858-552-9832
Fax: 858-535-3680
Email: [log in to unmask]
-----Original Message-----
From: DesignerCouncil [mailto:[log in to unmask]] On Behalf Of Dee Stover
Sent: Thursday, June 10, 2010 7:13 AM
To: [log in to unmask]
Subject: [DC] rohs, BGAs & assembly
Hi all,
I need to find some written data on the long term reliability of rohs
assemblies. We don't have comply with rohs but can only get the
parts in rohs, with BGA's being the main drive for rohs compliant solder.
Just had an assembly vendor say that a rohs bga can be assembled with
eutectic solder paste with good results. 2 other assembly shops say
that is not recommended. Is there any real studies or data available
that provides the real answer? Also studies and data for the
reliability of rohs? We need our boxes to work for 10 years or more.
Thank you for your time. What a great network for people to share
knowledge. I will also be going through PCD&F and google to
(hopelessly behind on my reading)
:-) Dee Stover [log in to unmask] 520-318-8489
Tech Associate II
National Optical Astronomy Observatories
www.noao.edu
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------------------------------------
DesignerCouncil Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To temporarily stop/(restart) delivery of DesignerCouncil send: SET DesignerCouncil NOMAIL/(MAIL)
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
---------------------------------------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------------------------------------
DesignerCouncil Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To temporarily stop/(restart) delivery of DesignerCouncil send: SET DesignerCouncil NOMAIL/(MAIL)
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
---------------------------------------------------------------------------------
|