TECHNET Archives

June 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 11 Jun 2010 17:50:12 +0200
Reply-To:
Subject:
From:
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; format=flowed; charset="iso-8859-1"; reply-type=original
MIME-Version:
1.0
Parts/Attachments:
text/plain (206 lines)
Does the solder paste have Silver adds?

Inge

--------------------------------------------------
From: "Bev Christian" <[log in to unmask]>
Sent: den 11 June 2010 17:40
To: <[log in to unmask]>
Subject: Re: [TN] Weird formation of voids

> Stewart,
> I lieu of a Dave Hillman Friday quiz, consider this it.  And you WIN! 
> Using an SEM and then carefully examining those pictures and the shape and 
> placement of the "voids" we were able to determine that it is exactly as 
> you describe.  We are now in the process of hitting our grinding paper 
> supplier "up the side of the head" for a crappy lot of product.
>
> Bev
> RIM
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Stewart McCracken
> Sent: Friday, June 11, 2010 11:36 AM
> To: [log in to unmask]
> Subject: Re: [TN] Weird formation of voids
> Importance: High
>
> Hi All,
>
> Looks as though sample preparation condition is less than ideal. Sample is 
> a little rounded and it appears that the voids might in fact be embedded 
> debris from the polishing equipment(?) I'm sure Vladimir would agree - get 
> it in the SEM to be sure! Need some better imaging and if possible EDS - 
> these will go a very long way to confirming what's going on. Lumps of 
> silicon carbide can really make a mess of a x-section. If you don't have 
> access to a SEM, you could etch the structure and look for abnormal 
> /unusual structures surrounding these features. Etching would also help to 
> refine the soft edges on a x-section (provide a more natural edge) and let 
> you see if you have shrinkage or gas voids (look at shape) filled with 
> grinding debris.
>
> Contaminated mats on a polishing station could explain the pattern of 
> occurrence and the feature. As always though, more info about condition 
> would make diagnosis easier!
>
> Kind regards,
>
> Stewart
>
> Stewart McCracken
> MCS Ltd.
> Centre House
> Midlothian Innovation Centre
> Roslin
> Midlothian
> EH25 9RE
>
> m. +44(0)7711 541735
> t.   +44(0)131 440 9090
> f.   +44(0)131 440 9085
> e.  [log in to unmask]
> w. www.themcsgroup.co.uk
>
>
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of stephen gregory
> Sent: 11 June 2010 16:21
> To: [log in to unmask]
> Subject: Re: [TN] Weird formation of voids
>
> Hi Bev!
>
> Got your picture today, and have it posted now:
>
> http://stevezeva.homestead.com/Bevs_Ball.jpg
>
> Almost looks like little pieces of dross. I wonder if something is going 
> on with the solder paste? Or leaded reflow profile with a lead-free BGA?
>
> Steve
>
> --- On Wed, 6/9/10, Bev Christian <[log in to unmask]> wrote:
>
>
> From: Bev Christian <[log in to unmask]>
> Subject: [TN] Weird formation of voids
> To: [log in to unmask]
> Date: Wednesday, June 9, 2010, 9:51 AM
>
>
> TechNetters,
> I am sending a picture to Steve to post.  I have labs in three locations. 
> One of them has seen weird voids in cross-sections of BGAs while the other 
> two locations have not.  For the lab that has seen them, the 
> cross-sections were prepared by different people on different days for 
> different products, using the same equipment. The voids are not in all 
> balls cross-sectioned but may be only in one of two of the balls in a row 
> of multiple solder joints examined.
>
> Have you seen anything like this?  Do you know the root cause?
>
> Vlad,
> You know what is going on, so please don't respond.
>
> Bev
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to 
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to 
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
> for additional information, or contact Keach Sasamori at [log in to unmask] or 
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to 
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to 
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
> for additional information, or contact Keach Sasamori at [log in to unmask] or 
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to 
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to 
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
> for additional information, or contact Keach Sasamori at [log in to unmask] or 
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------------------------
> This transmission (including any attachments) may contain confidential 
> information, privileged material (including material protected by the 
> solicitor-client or other applicable privileges), or constitute non-public 
> information. Any use of this information by anyone other than the intended 
> recipient is prohibited. If you have received this transmission in error, 
> please immediately reply to the sender and delete this information from 
> your system. Use, dissemination, distribution, or reproduction of this 
> transmission by unintended recipients is not authorized and may be 
> unlawful.
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to 
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to 
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
> for additional information, or contact Keach Sasamori at [log in to unmask] or 
> 847-615-7100 ext.2815
> -----------------------------------------------------  


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2