I've uploaded some pictures here:
http://ipc-technet.groupsite.com/gallery/13697
These are solder sleeves, and I'm wondering if they're rejectable per J-STD-001 Rev. E para. 5.1.2 (for Class 3), which now says:
"There shall [A1D2D3] be no strand separation (birdcaging) greater than one strand diameter or beyond the outside diameter of the insulation."
I've always considered birdcaging to be strands that are separated out and away from the other strands, leaving an air gap, like we see in the pictures in IPC-A-610. But in this case, these strands are separated at an angle radially with respect to the lay of the other strands.
Now 610E has a defect for "The general spiral lay of the strands has not been maintained", but there isn't anything similar in J-1.
I'm probably on shaky ground here because I don't really understand why birdcaging is a defect in the first place. Does it lead to early fatigue failure in the wire? And if that's the reason, would we see the same problem with the condition in these pictures? Should we care whether all strands run parallel?
-Joe
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|