Lon,
I would not for a second rely upon such a construction. You can not torque
adequately, because of so few active threads, and also because the FR4
material is not mechanically stable , especially not when exposed to temp
cycling. The heavier the block, the less reliable. Can't see what's the
problem with std washer and nut on the solder side?
Inge
--------------------------------------------------
From: "Lon Weffers" <[log in to unmask]>
Sent: den 17 June 2010 09:43
To: <[log in to unmask]>
Subject: [TN] Screwing earthrail into pcb FR4
> Dear all,
>
> For a customer we have to screw an earthrail (8 cable entries with screws
> M3x6, block is about 6cm long) on the componentside of the board. He uses
> 2
> "taptide" M4x12 screws, mounted with the head on top of the earthrail,
> through the rail, into the FR4 material (1,6mm)
> There is no nut on the solderside.
>
>
> In my opinion this isn't a reliable construction. Does any of you have
> some
> experience or remarks concerning this matter?
>
> Regards
>
> Lon Weffers
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|