TECHNET Archives

June 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Ioan Tempea <[log in to unmask]>
Date:
Thu, 17 Jun 2010 09:47:28 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Mike Sewell <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
Mike Sewell <[log in to unmask]>
Parts/Attachments:
text/plain (193 lines)
Linda,

Which 3M tape are you using?  Some of their low charge generating Kapton tapes have a low residue acrylic adhesive, and are not residue free.

I think ATS-667 is the same as the old Humitape.  They sell direct and can custom slit to your width from the log.  http://www.ats24.com  It is also sold by All-Spec under the Dadas tapes line. Rubber adhesive (not silicone) gives sharp mask lines.  No issues with residue for us.

Mike 


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ioan Tempea
Sent: Thursday, June 17, 2010 9:36 AM
To: [log in to unmask]
Subject: Re: [TN] 3M tape/adhesive concern

Hi,

Don't know if these residues pass IPC-610, but they are a disaster for conformal coating!

As per 3M spec, the Kapton tape has a max temperature of 500F. Does it see more than this in your process?

Regards,

Ioan Tempea, ing.
Ingénieur Principal de Fabrication / Senior Manufacturing Engineer
T | 450.967.7100 ext.244
E | [log in to unmask] 
W | www.digico.cc

N'imprimer que si nécessaire - Print only if you must

-----Message d'origine-----
De : Steve Gregory [mailto:[log in to unmask]] 
Envoyé : June-17-10 8:38 AM
À : [log in to unmask]
Objet : Re: [TN] 3M tape/adhesive concern

Hi Linda!

 

Gosh, I'm sorry I didn't get these posted earlier. I was planning to as soon
as I got them, but I got busy doing something else and forgot about your
request. Thanks for reminding me.

 

Anyways, here's your pictures:

 

http://stevezeva.homestead.com/adhesive.JPG

 

http://stevezeva.homestead.com/adhesive_2.JPG

 

http://stevezeva.homestead.com/paper_debri.JPG

 

http://stevezeva.homestead.com/under_button.JPG

 

I know it's bit of a challenge to find good conformal coat masking tape that
doesn't leave residues and debris, especially if you bake the boards to tack
cure the coating.

 

I don't know why Humiseal quit making their tape, it was one of the best
tapes I ever used. But then they just stopped making it for some reason.

 

Steve

 

From: Linda Langley [mailto:[log in to unmask]] 
Sent: Monday, June 14, 2010 2:43 PM
To: Steve Gregory
Subject: FW: 3M tape/adhesive concern

 

Steve,

Could you please post these pictures? We are having problems where there is
adhesive is sticking to the board when we pull the tape off.

Does anyone know if this would be a problem according to IPC? Would this be
considered Particulate Matter? Any info will be greatly appreciated.

 

Thanks

 

Linda Langley CIT

Training Specialist

Jabil Circuit

248-292-6176

From: Klara Szalay 
Sent: Tuesday, June 08, 2010 8:23 AM
To: Linda Langley
Subject: RE: 3M tape

 

I am sorry, I had to leave early yesterday. Here are some pictures of what
you looked at yesterday. Let me know if you need additional pictures.

Klara

 

From: Linda Langley 
Sent: Monday, June 07, 2010 10:37 AM
To: Klara Szalay
Subject: 3M tape

 

Klara,

Can you send me a picture of the tape concern?

 

Linda Langley CIT

Training Specialist

Jabil Circuit

248-292-6176



______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2