Bon jour Dominic,
It needs to be higher than for SnPb, but only by about 30 to 40C.
Werner
-----Original Message-----
From: Dominic Boudreau <[log in to unmask]>
To: [log in to unmask]
Sent: Wed, May 5, 2010 2:29 pm
Subject: [TN] Lead free hand soldering
Hello Technetters, I have two questions for you regarding lead-free hand
soldering :
1) What is the iron temperature range that you use to hand solder lead free
wire solder (SAC305)?
2) Do the iron temperature should be set higher for a lead free wire
solder? Some people say that the iron temperature should be the same for lead
and lead-free wire solder and some say that the temperature should be 50 °F
higher for lead-free.
I know that the iron temperature depends on many factors, but I just would like
to have a general idea.
Any comments would be much appreciated.
Dominic Boudreau, ing.
Ingénieur de produit / Manufacturing Engineer
E | [log in to unmask] <mailto:[log in to unmask]>
W | www.digico.cc <http://www.digico.cc/>
N'imprimer que si nécessaire - Print only if you must
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|