Toby,
I have been there and done that, believe me you don't want to be there!
You also need to apply etchant resist, probably using photo resist. I
played with Kodak KPR years ago, you also need a solvent to strip unexposed
resist. You also need the light source. And we have not talked about
drilling. You can purchase pre-sensitized PCB material but that is not free.
My dad never "Appreciated" the local electric utility. About 5 years ago a
bad hurricane came up the US east coast (I am in Baltimore) and he lost
power. He has a farm and needed electricity so I setup a generator. After 1
week of filling that thing with gasoline and computing the cost (He is a
farmer but he also has a PhD in Civil Engineering.) he is more attuned to
the benefits of paying the electric bill.
As I look at the prices charged by Olimex and the others I almost feel
guilty about what I get and how much I paid. I would never attempt to do it
on my own again.
Give me a call at 410-821-1315. Way back in the 70's I had built my own
process camera, KPR sprayer, developer trays, tin lead plating tank, etcher
and small drill. Don't Do It.
Bob Kondner
410-821-1315
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Toby Carrier
Sent: Friday, May 14, 2010 9:54 AM
To: [log in to unmask]
Subject: Re: [TN] Hobbyist PCB Fab Equipment
John,
I am not based in California, I am in Kentucky. I would be dealing with
line/spacing of about 10mils. I am just wanting to make small to medium
sized boards for hobbyist projects. Most of the boards would be single
sided, maybe a few double sided.
I had read about heating up the ferric acid to make the etching process
faster, but after just coming out of a chemistry class, I didn't like the
approach!!! If it takes 30mins, then it will have to take 30mins, I can
wait!!!
I have used a couple of previous mentioned board houses, but it cost more
money after tooling costs to than it would have just to get a setup for
making small boards at home. But, if I do decide to make it a professional
grade board, then I will fork out the money and have it fabricated
elsewhere.
Thanks for all the info.
Toby
On Thu, May 13, 2010 at 10:47 PM, John Burke <[log in to unmask]> wrote:
> Toby I am praying you are not based in California.....8-)
>
> I have made boards this way using ferric chloride but that was nearly 35
> years ago - it can be very health hazardous if approached incorrectly to
> give an example I knew a guy who read it would be better with hotter
ferric
> chloride so he put it on the stove, he had to buy his wife a new stove
> after
> the first couple of months as the old one "corroded in place".
>
> You have not stated what line/space you will be using as you might get
some
> better direction with this information.
>
> I think everyone on the link has taken it as given that these boards are
> either single or double sided........8-)
>
> Strongly suggest that you price out your projects with some of the proto
> shops that others on the link have mentioned unless of course you are
doing
> this for fun?...and do bear in mind with surface mount you may do better
> with those shops unless you intend setting up printing solder resist
> yourself?
>
> Best regards,
>
> John
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Toby Carrier
> Sent: Thursday, May 13, 2010 10:06 AM
> To: [log in to unmask]
> Subject: [TN] Hobbyist PCB Fab Equipment
>
> Hello all,
>
> I want to start making PCB's at home for prototyping small to medium
> projects, but I have a few questions about materials, kits and equipment:
>
> 1. What is the best kit to buy?
> 2. What equipment do I need?
> 3. Where is the best place to get the equipment and/or kits?
> 4. What safety hazards do I need to worry about?
>
> I will be dealing with through-hole and surface mount parts.
>
> Thanks for the help.
>
> Toby Carrier
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
>
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|