Scott,
I can think of multiple directions your process may take you, depending
other attributes of the part.
Not sure just how much actual brazing you will be doing with one component
being tin plated. Maybe you just want a higher temp solder than the normal
SnPb or SAC solders.
I would certainly work with Indium for preforms and pastes, SPM for precious
metal preforms, and Handy & Harmen for pastes and performs.
I would be greatly surprised if you had to go anywhere else to get the
assistance you required.
If your project just required a higher temp solder alloy, like a 300+°C
high-lead alloy, that will open you up to a whole slew of other solder mfrs
as well.
Hope this helps a bit.
Steve Creswick
http://www.linkedin.com/in/stevencreswick
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Post, Scott E
Sent: Thursday, May 13, 2010 12:46 PM
To: [log in to unmask]
Subject: [TN] Sources of brazing materials
I have an application for resistance brazing, which is new territory for
me. I'll be brazing a Sn plated Cu leadframe to a rather thick (0.062")
copper bracket which may or may not also be plated. Can anyone point me
towards reputable suppliers of brazing materials? Hopefully a supplier
with good apps engineering support to help bring me up the learning
curve. Google turns up quite a few sources, so I'm hoping to narrow the
field some with recommendations from you folks.
Scott Post
Staff Manufacturing Engineer
P.O.U. 0000-001E-0CTC
2151 E. Lincoln Road
Kokomo, Indiana 46904-9005
765-451-2983 (Phone)
765-451-0287 (FAX)
****************************************************************************
************
Note: If the reader of this message is not the intended recipient, or an
employee or agent responsible for delivering this message to the intended
recipient, you are hereby notified that any dissemination, distribution or
copying of this communication is strictly prohibited. If you have received
this communication in error, please notify us immediately by replying to the
message and deleting it from your computer. Thank you.
****************************************************************************
************
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|