Hi Leland - one thing to keep in mind that absorption rates are going to
be different for exposure to liquid water than water vapor . If you had
exposed your test components to steam instead of liquid water, you most
likely would have had a different result. The difference in absorption
rates is one of the reasons that we can clean a printed wiring assembly
between reflow pass top and reflow pass bottom without suffering
significant popcorning events. Also, plastics have different
susceptibility to water absorption so you may have had a plastic that was
robust against water intrusion.
Dave
Leland Woodall <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
05/26/2010 02:31 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Leland Woodall <[log in to unmask]>
To
[log in to unmask]
cc
Subject
[TN] MSD Devices and Popcorning
Just on a note of curiosity, how many folks out there are using a
sophisticated RFID process to track their MSD exposure times?
We're using a manual system, and lately I've had a couple of people
inquiring about moving to something much more expensive. In my ten
years here, we've never seen either an internal nor external failure due
to popcorning, micro cracks in our devices, or anything along those
lines.
A few years ago, I took 10 scrap ICs and soaked them in a glass of water
over a four day weekend. When we returned on a Tuesday, I pulled them
out, dried the surfaces off, and sent them through a lead free process
reflow oven on a bare board.
After everything I'd read and investigated, I expected them to explode.
I performed an intense examination of both sides of the components under
100X magnification, and I was extremely surprised to see no incidents of
popcorning nor package cracks. I then checked them in our X-ray
machine, and saw no evidence of any bond wire detachments.
Has anyone conducted a similar experiment with dissimilar results?
I'm just wondering if we're making a mountain out of a mole hill here...
Thanks,
Leland
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|