Bev,
I had the same q some time ago in conjuntion with epoxy bleedout. We
suspected leakage of Bisphenol, which is not healthy in electronics. Asked
a glue sniffer at Loctite (Henkel) and he replied that nearly all epoxies
contain Bisphenol A. Alternatives exist but are not of commercial interest,
he said.
Inge
--------------------------------------------------
From: "Bev Christian" <[log in to unmask]>
Sent: den 14 May 2010 03:11
To: <[log in to unmask]>
Subject: Re: [TN] Halogen free laminate chemistry
> Denny,
> Thanks for answering, you are the first so far.
>
> You forgot you can't attach things to TechNet messages. Send the white
> paper to me directly, please.
>
> Our boards have been halogen free for years, but it had nothing to do with
> environmental considerations.
>
> Do all epoxies by definition have to contain bisphenol A?
>
> Bev
>
>
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Dennis Fritz
> Sent: Thursday, May 13, 2010 8:29 PM
> To: [log in to unmask]
> Subject: Re: [TN] Halogen free laminate chemistry
>
> I think all halogen free laminates are tetra-bromo-bisphenol-A free.
> However, bisphenol-A is the co-momomer for epoxy, so if they are FR-4
> (epoxy) they must still contain bisphenol-A. I think for flammability
> (pass
> UL 94-V0) the additives are aluminum oxide, nitrogen or phosphorus
> containing organics, etc.
>
> I have attached the original IPC white paper on halogen free from 2002. I
> understand a lot of this was "voted down", as IPC wanted to take a
> different
> stance toward halogen free for Intel, Dell, HP, and others - who supply
> computers graded to the E-Peat scale, where halogen free is a major
> objective.
>
> Is RIM now into making "my hand-held is greener than your hand-held"
> products? I guess my view that "halogen-free is bad science" attitude is
> showing through.
>
> Denny
>
>
>
>
>
>
> -----Original Message-----
> From: Bev Christian <[log in to unmask]>
> To: [log in to unmask]
> Sent: Thu, May 13, 2010 2:19 pm
> Subject: [TN] Halogen free laminate chemistry
>
>
> Are all halogen free laminates bisphenol A free?
> ev
> IM
> ---------------------------------------------------------------------
> his transmission (including any attachments) may contain confidential
> nformation, privileged material (including material protected by the
> olicitor-client or other applicable privileges), or constitute non-public
> nformation. Any use of this information by anyone other than the intended
> ecipient is prohibited. If you have received this transmission in error,
> please
> mmediately reply to the sender and delete this information from your
> system.
>
> se, dissemination, distribution, or reproduction of this transmission by
> nintended recipients is not authorized and may be unlawful.
> ______________________________________________________________________
> his email has been scanned by the MessageLabs Email Security System.
> or more information please contact helpdesk at x2960 or [log in to unmask]
> _____________________________________________________________________
> ---------------------------------------------------
> echnet Mail List provided as a service by IPC using LISTSERV 15.0
> o unsubscribe, send a message to [log in to unmask] with following text in
> he BODY (NOT the subject field): SIGNOFF Technet
> o temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> o receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> earch the archives of previous posts at: http://listserv.ipc.org/archives
> lease visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for
> dditional information, or contact Keach Sasamori at [log in to unmask] or
> 47-615-7100 ext.2815
> ----------------------------------------------------
>
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|