TECHNET Archives

May 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 7 May 2010 19:01:08 +0200
Reply-To:
Subject:
From:
Content-Transfer-Encoding:
8bit
In-Reply-To:
Content-Type:
text/plain; format=flowed; charset="iso-8859-1"; reply-type=original
MIME-Version:
1.0
Parts/Attachments:
text/plain (125 lines)
Ioan,
I think I know what's smoking...it's the CAFfein.
Inge
--------------------------------------------------
From: "Ioan Tempea" <[log in to unmask]>
Sent: den 7 May 2010 18:07
To: <[log in to unmask]>
Subject: Re: [TN] Wrinkling of conformal coating

> In case you guys thought you got away by talking about alien espresso 
> machines, I have one more question.
>
> Took a bare board from stores and stuck it into the reflow oven. I have 
> noticed smoke coming out from the tunnel while the PCB was in. Not huge or 
> thick, but just enough smoke to notice it. Could this mean anything 
> regarding the board, like not cured something, poor FR-4 or else?
>
> Thanks,
>
> Ioan Tempea, ing.
> Ingénieur Principal de Fabrication / Senior Manufacturing Engineer
> T | 450.967.7100 ext.244
> E | [log in to unmask]
> W | www.digico.cc
>
> N'imprimer que si nécessaire - Print only if you must
>
>
>
> Dear Technos,
>
>
>
> Back to orange peeling, this time concerning conformal coating, please see
> http://ipc-technet.groupsite.com/galleries/photo/124230
>
>
>
> The coating is applied with an Asymtek Century machine and is a Conap 1170
> acrylic.
>
>
>
> ˇ         The board is left curing in ambient temperature, no
> acceleration. Starting with an even coating, in about 20-30 minutes the
> liquid seems to move towards a certain area (no rippling at this moment).
> After another 10-15 minutes the rippling effect sets in.
>
> ˇ         We thought that due to the almost 2 minutes lag between the
> coating of the first and last image, the drying of the coating layer is
> not even and the one side curing first pulls on the liquid at the other
> end. So we've cut the panel in 2, accelerated the machine, the problem is
> still there.
>
> ˇ         The boards are laid as flat as possible, maybe not perfectly
> horizontal, but not worse than others with the same coating, that do not
> show any issue
>
> ˇ         Just to make it more difficult: grabbed a non-populated panel
> from the stores, coated it, placed on the same flat surface, and guess
> what: no issues.
>
>
>
> The PCB has Taiyo PSR 4000 MP soldermask.
>
>
>
> So I would need your guidance in clarifying where is this coming from and
> how to fix it.
>
>
>
> Thank you,
>
>
>
> Ioan Tempea, ing.
> Ingénieur Principal de Fabrication / Senior Manufacturing Engineer
> T | 450.967.7100 ext.244
> E | [log in to unmask] <mailto:[log in to unmask]>
> W | www.digico.cc <http://www.digico.cc/>
>
>
> N'imprimer que si nécessaire - Print only if you must
>
>
>
>
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to 
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to 
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
> for additional information, or contact Keach Sasamori at [log in to unmask] or 
> 847-615-7100 ext.2815
> -----------------------------------------------------  


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2