Torsten,
pH13!!! None of the ordinary polymers will withstand that. Are you sure of
the requirement? I've never seen anything like that. I don't think even
Parylene will be enough. I used Parylene C for military encapsulation of
parts that had to pass salt spray for weeks, high temperatures and like, and
we found that to withstand such a harsh environment , the Parylene had to be
so thick, that the process had to be modified. The cost per package had been
quite unrealistic.
I would try ceramic spraying, that's probably your solution. There are lots
of variants. I can't tell you which one suits best. Some are for
electronics, others not. You better check the below URL and call the
respective ceramic spray specialist.
http://www.electronics.ca/publications/products/Coatings-for-Medical-Devices-%252d-Global-Strategic-Business-Report.html
Good Luck
Inge
--------------------------------------------------
From: "Torsten Hagge" <[log in to unmask]>
Sent: den 25 May 2010 12:30
To: <[log in to unmask]>
Subject: [TN] Coating
> Hi Technetters,
>
> looking for an conformal coating for electronics used in medical
> application. The small electronic should be able to pass 1000 cycles
> washing and cleaning process with ph=13 plus 20 minutes autoclave 135°C @
> 2bar.
>
> 1st idea is parylene coating, any cheaper or better ideas?
>
> Regards,
> Torsten
>
> Dipl.Ing.(FH)Torsten Hagge
> tech. projectmanager
> Kristronics GmbH
> Gewerbegrund 5 - 9
> 24955 Harrislee
>
> Tel.: +49 461 7741 624
> Fax: +49 461 7741 642
> [log in to unmask]
> www.kristronics.de
>
> Gerichtsstand Flensburg, Handelsregister: HRB 1433 FL
> Geschäftsführer Dipl.-Ing. oec. Thormod Ohm
> Ust-Id-Nr. DE 811182059
> Bankverbindung: Deutsche Bank AG Flensburg, Konto-Nr. 4216610, BLZ
> 21570011
> IBAN: DE32 2157 0011 0421 6610 00, BIC: DEUT DE HH 215
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|