Mike, can you decifer your high english in the last line, so that a poor
non- linguistic- elite creature can understand.
Your magniloquence is incommensurable, sir.
Inge
--------------------------------------------------
From: "Mike Fenner" <[log in to unmask]>
Sent: den 4 May 2010 15:51
To: <[log in to unmask]>
Subject: Re: [TN] Question about Voids in Solder Joints
> I don't think this is an entirely rational zone, so data will be ignored
> as
> required.
>
> Personally I think the problem with voiding is that people see a process
> variable and confuse that with a functional requirement, not realising
> that
> solder joints are usually well over size for strength and conductivity,
> and
> are arbitrarily sized anyway.
>
> This means even if there were no relationship with
> reliability/functionality
> a large variation in voiding would still be seen as bad. The fact that up
> to 75% of the solder joint need not be there is irrelevant to a mind used
> to working with and therefore conditioned by plus minus single digit
> tolerances/ppm>ppb faults on a line.
>
>
>
> Regards
>
> Mike
>
>
> * Please think before you print
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Inge
> Sent: Tuesday, May 04, 2010 2:11 PM
> To: [log in to unmask]
> Subject: Re: [TN] Question about Voids in Solder Joints
>
> You speak about so and so percentage of voíds in the SJs. Bart Vandevelde
> presented, a number of years ago, results from evaluation of solder joint
> void in CSP. FC, BGA and the void size vs. strain during temp cycling.
> Voids as big as 75 % did not cause significant stress, while a number of
> very small voids caused noticable stress, namely, because they were
> adjacent
>
> to each other, in a row, so as to say. So maybe one stops packages with
> a
> large void and lets go a package with a number of small voids.
>
> Inge
>
> --------------------------------------------------
> From: "Bev Christian" <[log in to unmask]>
> Sent: den 4 May 2010 14:22
> To: <[log in to unmask]>
> Subject: Re: [TN] Question about Voids in Solder Joints
>
>> Underway. THAT I will not be able to share.
>> Bev
>> RIM
>>
>> -----Original Message-----
>> From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor Hernandez
>> Sent: Tuesday, May 04, 2010 8:01 AM
>> To: [log in to unmask]
>> Subject: Re: [TN] Question about Voids in Solder Joints
>>
>> Was a deep dive conducted on field return fsilure to attribute the
>> failure to leaded component voiding?
>>
>> Victor,
>>
>> -----Original Message-----
>> From: TechNet [mailto:[log in to unmask]] On Behalf Of Bev Christian
>> Sent: Monday, May 03, 2010 7:24 PM
>> To: [log in to unmask]
>> Subject: Re: [TN] Question about Voids in Solder Joints
>>
>> Thanks, George. Most detailed answer yet.
>>
>> At Nortel we never had a void spec for leaded components either. And, as
>> I
>> think I have said on TechNet before, we would find many joints after
>> pull
>> testing or cross-sectioning that looked like Swiss cheese, but we never
>> had
>> field failures as a result. BUT we were manly concerned about the
>> possibility of failures due to thermal cycling.
>>
>> Now I worked for a company where the main concern is customers dropping
>> their product onto hard edges. We do a lot of work to try and design
>> and
>> build products to survive multiple drops in different orientations, but
>> occasionally a switch is going to come down on a pointed rock or a
>> customer
>> is going to rip a charging cable out of a connector at a 45 degree angle
>> (yikes). These are the things I am talking about. I was leaning
>> towards
>> 25% for leaded components, so you and I are in the same ball park,
>> George.
>> Others have suggested a higher number, but without some encouraging
>> words in
>> that direction from fellow TechNetters, I ain't goin' there.
>> Bev
>> RIM
>>
>> -----Original Message-----
>> From: TechNet [mailto:[log in to unmask]] On Behalf Of Wenger, George M.
>> Sent: Monday, May 03, 2010 5:57 PM
>> To: [log in to unmask]
>> Subject: Re: [TN] Question about Voids in Solder Joints
>>
>> Bev,
>>
>> We're in a similar position to Dave Hillman. We basically follow IPC
>> standards (where there are standards). We do not have a company
>> standard
>> for leaded components. A couple of small voids is okay, more or large
>> voids
>> are not. Having said that you'll probably ask how many is a couple and
>> what
>> is small and what is large. We don't have a really good answer. Since
>> we
>> do a lot of RF power component work we've adopted a voiding
>> specification
>> that has worked well for IC packages. They typically use a criteria of
>> total die attach voids <20% with no single void >5% is okay. We don't
>> actually measure voids in leaded devices but if we were to see 20%
>> voiding
>> in a leaded component solder joint we'd be concerned.
>>
>> Regards,
>> George
>> George M. Wenger
>> Senior Principal FMA / Reliability Engineer
>> Andrew Corporation - Wireless Network Solutions
>> 40 Technology Drive, Warren, NJ 07059
>> (908) 546-4531 Office (732) 309-8964 Mobile
>> E-mail: [log in to unmask]
>> -----Original Message-----
>> From: TechNet [mailto:[log in to unmask]] On Behalf Of Bev Christian
>> Sent: Monday, May 03, 2010 3:48 PM
>> To: [log in to unmask]
>> Subject: [TN] Question about Voids in Solder Joints
>>
>> TechNetters,
>> I was thinking about just putting "Voiding" as the e-mail title, but I
>> contemplated what I might get in responses and amended my title
>> accordingly.
>>
>> My question is the following: do any of your companies have upper limits
>> on the amount of voiding in SMT solder joints of components that
>> customers have access to - like connectors and switches? These of
>> course are leaded components. I am not talking about Pb, but the form
>> of the interconnect between the component body and the board.
>>
>> If so, are you willing and can you share?
>>
>> Bev
>> RIM
>>
>> ---------------------------------------------------------------------
>> This transmission (including any attachments) may contain confidential
>> information, privileged material (including material protected by the
>> solicitor-client or other applicable privileges), or constitute
>> non-public
>> information. Any use of this information by anyone other than the
>> intended
>> recipient is prohibited. If you have received this transmission in
>> error,
>> please immediately reply to the sender and delete this information from
>> your
>> system. Use, dissemination, distribution, or reproduction of this
>> transmission by unintended recipients is not authorized and may be
>> unlawful.
>>
>> ______________________________________________________________________
>> This email has been scanned by the MessageLabs Email Security System.
>> For more information please contact helpdesk at x2960 or
>> [log in to unmask]
>> ______________________________________________________________________
>>
>> ---------------------------------------------------
>> Technet Mail List provided as a service by IPC using LISTSERV 15.0
>> To unsubscribe, send a message to [log in to unmask] with following text
>> in
>> the BODY (NOT the subject field): SIGNOFF Technet
>> To temporarily halt or (re-start) delivery of Technet send e-mail to
>> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>> To receive ONE mailing per day of all the posts: send e-mail to
>> [log in to unmask]: SET Technet Digest
>> Search the archives of previous posts at:
>> http://listserv.ipc.org/archives
>> Please visit IPC web site
>> http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>> for additional information, or contact Keach Sasamori at [log in to unmask]
>> or
>> 847-615-7100 ext.2815
>> -----------------------------------------------------
>>
>> ______________________________________________________________________
>> This email has been scanned by the MessageLabs Email Security System.
>> For more information please contact helpdesk at x2960 or
>> [log in to unmask]
>> ______________________________________________________________________
>>
>> ---------------------------------------------------
>> Technet Mail List provided as a service by IPC using LISTSERV 15.0
>> To unsubscribe, send a message to [log in to unmask] with following text
>> in
>> the BODY (NOT the subject field): SIGNOFF Technet
>> To temporarily halt or (re-start) delivery of Technet send e-mail to
>> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>> To receive ONE mailing per day of all the posts: send e-mail to
>> [log in to unmask]: SET Technet Digest
>> Search the archives of previous posts at:
>> http://listserv.ipc.org/archives
>> Please visit IPC web site
>> http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>> for additional information, or contact Keach Sasamori at [log in to unmask]
>> or
>> 847-615-7100 ext.2815
>> -----------------------------------------------------
>>
>>
>> ______________________________________________________________________
>> This email has been scanned by the MessageLabs Email Security System.
>> For more information please contact helpdesk at x2960 or
>> [log in to unmask]
>> ______________________________________________________________________
>>
>> ---------------------------------------------------
>> Technet Mail List provided as a service by IPC using LISTSERV 15.0
>> To unsubscribe, send a message to [log in to unmask] with following text
>> in
>> the BODY (NOT the subject field): SIGNOFF Technet
>> To temporarily halt or (re-start) delivery of Technet send e-mail to
>> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>> To receive ONE mailing per day of all the posts: send e-mail to
>> [log in to unmask]: SET Technet Digest
>> Search the archives of previous posts at:
>> http://listserv.ipc.org/archives
>> Please visit IPC web site
>> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
>> information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
>> ext.2815
>> -----------------------------------------------------
>>
>> ______________________________________________________________________
>> This email has been scanned by the MessageLabs Email Security System.
>> For more information please contact helpdesk at x2960 or
>> [log in to unmask]
>> ______________________________________________________________________
>>
>> ---------------------------------------------------
>> Technet Mail List provided as a service by IPC using LISTSERV 15.0
>> To unsubscribe, send a message to [log in to unmask] with following text
>> in
>> the BODY (NOT the subject field): SIGNOFF Technet
>> To temporarily halt or (re-start) delivery of Technet send e-mail to
>> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>> To receive ONE mailing per day of all the posts: send e-mail to
>> [log in to unmask]: SET Technet Digest
>> Search the archives of previous posts at:
>> http://listserv.ipc.org/archives
>> Please visit IPC web site
>> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
>> information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
>> ext.2815
>> -----------------------------------------------------
>>
>> ---------------------------------------------------------------------
>> This transmission (including any attachments) may contain confidential
>> information, privileged material (including material protected by the
>> solicitor-client or other applicable privileges), or constitute
>> non-public
>
>> information. Any use of this information by anyone other than the
>> intended
>
>> recipient is prohibited. If you have received this transmission in error,
>> please immediately reply to the sender and delete this information from
>> your system. Use, dissemination, distribution, or reproduction of this
>> transmission by unintended recipients is not authorized and may be
>> unlawful.
>>
>> ______________________________________________________________________
>> This email has been scanned by the MessageLabs Email Security System.
>> For more information please contact helpdesk at x2960 or [log in to unmask]
>> ______________________________________________________________________
>>
>> ---------------------------------------------------
>> Technet Mail List provided as a service by IPC using LISTSERV 15.0
>> To unsubscribe, send a message to [log in to unmask] with following text in
>> the BODY (NOT the subject field): SIGNOFF Technet
>> To temporarily halt or (re-start) delivery of Technet send e-mail to
>> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>> To receive ONE mailing per day of all the posts: send e-mail to
>> [log in to unmask]: SET Technet Digest
>> Search the archives of previous posts at:
>> http://listserv.ipc.org/archives
>> Please visit IPC web site
>> http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>
>> for additional information, or contact Keach Sasamori at [log in to unmask]
>> or
>
>> 847-615-7100 ext.2815
>> -----------------------------------------------------
>
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
>
> ***This email, its content, and any files transmitted with it, are
> intended solely for the addressee(s) and may be legally privileged and/or
> confidential. If you are not the intended recipient, please contact the
> sender by return and delete the material from any computer. Any review,
> retransmission, dissemination, or other use of, or taking of any action in
> reliance upon this information by persons or entities other than the
> intended recipient is prohibited.
>
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|