Well, we avoided it as long as we could, but now I have to design for RoHS
compliance.
I'm basically following Werner's recommendations (which don't conflict with
anyone else's as far as I know), but I'm confused about one aspect of
material:
Several sources have stated that its better to use "NON-DICEY" material, but
none of the IPC-4101 slash sheets mention dicy or non-dicy (or
dicyandiamide).
If we are trying /126 material, do we still have to specify non-dicy?
thanks,
Jack
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|