Linda,
It is very clear that they are not the original samtec parts. The potting of the connector housing is very bad especially when you mentioned that the leads and sides fall apart when removed.
IPC/WHMA-A-620 : Requirements and Acceptance for Cable and Wire Harness Assemblies has a few pages under Section 10 to take care of molding/potting for the connectors. It is a reject for all classes as long as the followings are found :
- voids where molding material should be present
- marking is incomplete or not legible
- incomplete material fill
- exposed insulation, sleeving, jacket, braid or foil.
Hope the information give you some insight to make your decision.
Thanks and Regards,
~ Wee Mei ~
________________________________
From: TechNet on behalf of Linda Langley
Sent: Thu 5/13/2010 8:33 PM
To: [log in to unmask]
Subject: [TN] FW: Connector issue
Steve has posted a picture for me and I would greatly appreciate any
information anyone can share. The vendor says the connectors meet IPC
Standards.
Does anyone know of an IPC Standard that would address this issue?
Thank You Steve.
Linda Langley CIT
Training Specialist
Jabil Circuit
248-292-6176
From: Steve Gregory [mailto:[log in to unmask]]
Sent: Thursday, May 13, 2010 8:20 AM
To: Linda Langley
Subject: RE: Connector issue
Hi Linda!
It's up! Go to:
http://stevezeva.homestead.com/Connector_SSW-101-01-S-T.ppt
Steve
From: Linda Langley [mailto:[log in to unmask]]
Sent: Thursday, May 13, 2010 8:06 AM
To: Steve Gregory
Subject: FW: Connector issue
Steve,
Could you please post this picture? We are having an issue where the
vendor is saying they meet IPC Standards but I don't know of a standard
that would address this problem.
Maybe someone can point me in the right direction for information.
Linda Langley CIT
Training Specialist
Jabil Circuit
248-292-6176
From: Justin Hartley
Sent: Wednesday, May 12, 2010 2:29 PM
To: Linda Langley
Subject: Connector issue
Thank you,
Justin Hartley
Supplier Quality Engineer
3800 Giddings Rd.
Auburn Hills, MI 48326
Ph: 248-292-6220
F: 248-292-6922
Cell: 248-320-3271
[log in to unmask]
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|