I have always found mud and bare feet to work well. Then plaster casts to
measure the footprints.
Doug Pauls
"Braddock, Iain (UK)" <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
05/06/2010 10:04 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
"Braddock, Iain (UK)" <[log in to unmask]>
To
[log in to unmask]
cc
Subject
[TN] Footprints?
Hi everyone,
Just a quick straw pole. I am trying to gauge what this community are
using to generate footprints.
IPC 7351_A (superseding IPC 782)? Some other international standard,
e.g. IEC 61188-5?, Bespoke footprints? A mixture of bespoke &
international standards?
Any feedback will be appreciated.
CIA,
Iain.
********************************************************************
This email and any attachments are confidential to the intended recipient
and may also be privileged. If you are not the intended recipient please
delete it from your system and notify the sender. You should not copy it
or use it for any purpose nor disclose or distribute its contents to any
other person.
MBDA UK Limited, a company registered in England and Wales, registration
number 3144919 whose registered office is at Six Hills Way, Stevenage,
Hertfordshire, SG1 2DA, England.
********************************************************************
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please visit http://www.messagelabs.com/email
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|