TECHNET Archives

May 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Thu, 27 May 2010 13:16:51 +0100
Reply-To:
Subject:
From:
Mike Fenner <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (141 lines)
What ever the theoretical merit of grounding/not grounding with respect to
metal drawers etc, not grounding allows an element of discretion on handling
ESD. It could be it is better to consistently apply SOP on grounding. It's
small steps between opening the drawer for a peek and then shuffling
contents around to see better, and then taking parts out...


Regards
 
Mike

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Lee Whiteman
Sent: Wednesday, May 26, 2010 7:50 PM
To: [log in to unmask]
Subject: Re: [TN] ESD spec question

Graham,

Every place I've worked at had a simple rule - if you are within 3 feet
of an ESD sensitive device, you have to be grounded.

These days, when in the cabinet you can have can contain Class 0
devices, whose threshold is about 250V, you do not want to run the risk
of damaging components by opening the cabinet while ungrounded.

To me, ESD and the X-Files define paranoia. Play it safe - be grounded.

Hope this helps. Good Luck.

Lee Whiteman, PMP
Senior Member Engineering Staff
L-3 Communications East
Telephone: (856) 338-3508
FAX: (856) 338-2906
E-Mail: [log in to unmask]
 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of
[log in to unmask]
Sent: Wednesday, May 26, 2010 12:30 PM
To: [log in to unmask]
Subject: [TN] ESD spec question

Hey TechNet
It's been a quiet day on Technet!  

I've got a question regarding ESD.  I was taught that if I am not
grounded I do not go near anything that is ESD .  The example we are
debating here today concerns parts that are stored in metal cabinets.
The cabinet is grounded, and within the cabinet drawers there are ESD
sensitive parts in individual bins, not covered or packaged (no faraday
cage).  

Is it OK to open the drawer and look into the cabinet without being
properly grounded?  I say no, but am I being overly cautious?

If "no" is the right answer, where would I find that in an ESD spec?
I've given ESD-S20.20 a quick peruse, nothing jumped out at me.

regards, 
  
Graham Collins 
Halifax Production Engineering 
(902) 873-2000 ext. 6215 

This message and any attachments are solely for the use of the
individual or entity to which it is addressed and may contain
information that is privileged or confidential or controlled technical
data that is subject to the laws of Canada or the United States. If you
are not the intended recipient, any disclosure, use or distribution of
the information contained herein is prohibited. If you have received
this communication in error, please notify the sender by reply e-mail
and immediately delete this message and any attachments.



______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


***This email, its content, and any files transmitted with it, are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient, please contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination, or other use of, or taking of any action in reliance upon this information by persons or entities other than the intended recipient is prohibited.

Messages sent via this medium may be subjected to delays, non-delivery, and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. Indium Corporation does not accept responsibility for changes made to this email after it was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.***


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2