TECHNET Archives

May 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Tue, 4 May 2010 11:06:10 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Roberts, Jon (SA-1)" <[log in to unmask]>
Subject:
From:
"Roberts, Jon (SA-1)" <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (110 lines)
Just reiterating what others have stated, Jon 


ANSI/ESD S20.20-2007 references the two mil spec below:

MIL-STD-1686, "Electrostatic Discharge Control Program for Protection of
Electrical and
Electronic Parts, Assemblies and Equipment (Excluding Electrically
Initiated Explosive Devices)"
MIL-HDBK-263, "Electrostatic Discharge Control Handbook for Protection
of Electrical and
Electronic Parts, Assemblies, and Equipment (Excluding
Electrically-Initiated Explosive Devices)"

Both 1686 and 263 are active Mil Spec.


Mil HDBK 263B the references Mil Std 1695:

40.1.17 Relative humidity. Humid air helps to dissipate electrostatic
charges by keeping surfaces moist, therefore increasing surface
conductivity.
Substantial electrostatic voltage levels can accumulate with a decrease
in
relative humidity (see appendix A, table IV). However, it is also
evident
from table IV that significant electrostatic voltages can still be
generated
with relative humidity as high as 90 percent. Relative humidity between
40
percent and 60 percent in ESD protective areas is desirable as long as
it does
not result in corrosion or in other detrimental effects such as PWB
delamination during soldering. Where high relative humidity levels
cannot be
maintained, ionized air can be used to dissipate electrostatic charges.
MIL-STD-1695 specifically addresses relative humidity control in the
context
of static electricity protection. The MIL-STD-1695 requirement is for
relative humidity levels in the range of 30-70 percent in areas where
electronic parts and hybrid microcircuits (MIL-STD-1695, work areas 5
and 6)
are handled or processed. MIL-STD-1695 requires the same level of
relative
humidity controls for handling and storage areas (MIL-STD-1695, work
area 13),
except when items are covered or protected.


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman
Sent: Tuesday, May 04, 2010 9:17 AM
To: [log in to unmask]
Subject: [TN] Mil Specification for Facility Humidity Requirements

Hi folks - my brain cells need an assist. I am looking for the military 
specification that calls out for a soldering facility to have a 30-60% 
humidity requirement. I know the IPC JSTD-001E paragraph 4.2.2 values
but 
also I remember a military specification also had the requirement but 
can't seem to find the document. 

TIA

Dave Hillman
Rockwell Collins 
[log in to unmask]


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

This communication is intended only for use by the addressee(s) named herein and may contain business confidential and/or legally privileged information. If you are not the intended recipient of this e-mail, you are hereby notified that any dissemination, distribution, disclosure or copying of this e-mail and its contents is strictly prohibited. If you have received this e-mail in error, kindly notify the sender by replying to this message. In addition, please permanently delete the message and any attachments without copying or disclosing the contents. Thank you for your cooperation.                                                                                                        
THIS DOCUMENT AND/OR SHIPMENT MAY CONTAIN COMMODITY ITEMS, SOFTWARE OR TECHNICAL DATA THAT IS CONTROLLED BY U.S. EXPORT LAW, AND MAY NOT BE EXPORTED OUTSIDE THE UNITED STATES OR TO NON U.S. PERSONS WITHOUT THE APPROPRIATE EXPORT LICENSE FROM EITHER THE U.S. DEPARTMENT OF STATE OR DEPARTMENT OF COMMERCE.

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2