TECHNET Archives

May 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Tharaka Chandanayaka <[log in to unmask]>
Date:
Fri, 21 May 2010 16:43:06 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Bev Christian <[log in to unmask]>
Subject:
From:
Bev Christian <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="iso-2022-jp"
MIME-Version:
1.0
Parts/Attachments:
text/plain (82 lines)
Tharaka,
I have never done this and make no claims as to the safety or usefulness of the methods I quickly found on the internet.  They all look nasty!

1) BCl3/HBr/Ar plasmas

2) and 3) Chemical etching of sapphire 
L. A. Marasina, V. V. Malinovsky, I. G. Pichugin, P. Prentky 
V. I. Uljanov (Lenin) Leningrad Electrical Engineering Institute, Leningrad, USSR
 Abstract 
The results on etching of sapphire substrates with different orientation are discussed. High temperature etching in hydrogen stream and etching in the mixture of H3PO4 and H2SO4 were used in experiments. 

4) SF6 plasma

5) Fabrication of wet-etched patterned sapphire substrates for
high-efficiency InGaN/GaN blue light-emitting diodes
C.-L. Wu, M.-H. Lo, Y.-L. Li
Graduate Institute of Photonics and Optoelectronics, National Taiwan University
No. 1, Sec. 4, Roosevelt Road, Taipei, 10617 Taiwan
Y.-C. Chang 
Two different etchants were used to
chemically etch the sapphire substrates: H2SO4
and a volume mixture of 3:1 H2SO4:H3PO4. The
sapphire substrates were immersed in the
etchant in a beaker and heated on a hot plate to
an etchant temperature from 260℃ up to 350℃.
   
6) Fused NaOH/KOH
      
   Bev
RIM
   
   
  
  
 
 


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Tharaka Chandanayaka
Sent: Friday, May 21, 2010 4:21 PM
To: [log in to unmask]
Subject: [TN] RE : Sapphire wafer etching

Hi everyone, 

I was wondering that anyone came across any methods that can etch Sapphire 
wafers in low temperatures. If know please let me know. Tech net is a great 
source of information.  

Thank you 
Tharaka Chandanayaka 
[log in to unmask] 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2