TECHNET Archives

May 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 21 May 2010 08:12:32 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Thayer, Wayne - IIW" <[log in to unmask]>
Subject:
From:
"Thayer, Wayne - IIW" <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (1814 lines)
But if DCTE x DT is in units of delta L/L, and I multiply that by another L, then final units of your equation are in L.

Something fails when stress (units of FORCE/(L x L)) exceeds a critical value.  To get to this unit you usually use elastic modulus, which is units of (FORCE/(L x L))/(L/L).  In a composite structure such as what we are talking about (part, board, solder), the overall elastic modulus is usually driven by the lowest elastic modulus in the system.

For a BGA, it is obvious that elastic modulus is unimportant, because the net resisting force of the balls (due to both relatively low elastic modulus and relatively large height) is so much less than the forces developed by the DCTE stress that we can assume it is negligible:  The balls will shear as dictated by your initial equation.  But for the QFN and LCC condition, my intuition causes me to wonder if the elastic modulus of the solder is also important, particularly since you pointed out in the paper I referenced earlier that the intermetallics due to very thin solder joints are much stronger than the bulk solder.

So should I interpret your response as the strength of the intermetallics is still not significant when analyzing QFN/LCC mountings?

Wayne

________________________________
From: Werner Engelmaier [mailto:[log in to unmask]]
Sent: Friday, May 21, 2010 7:35 AM
To: [log in to unmask]; Thayer, Wayne - IIW
Subject: Re: [TN] Solder joint height

DNP stands for distance from neutral point.
Werner



-----Original Message-----
From: Thayer, Wayne - IIW <[log in to unmask]>
To: [log in to unmask]
Sent: Fri, May 21, 2010 7:12 am
Subject: Re: [TN] Solder joint height

Thanks for your reply, Werner.










DNP?  I'm trying to figure that one out.  Something to do with elastic modulii?





Or is it number of cycles?










I got the 1.5mil number from the Amkor paper, BOARD LEVEL ASSEMBLY AND





RELIABILITY CONSIDERATIONS





FOR QFN TYPE PACKAGES.  Someone pointed that paper out on this forum a few





months ago.  That's why I decided to try the pin probe technique.










Wayne










________________________________





From: Werner Engelmaier [mailto:[log in to unmask]<mailto:[log in to unmask]>]





Sent: Thursday, May 20, 2010 6:30 PM





To: [log in to unmask]<mailto:[log in to unmask]>; Thayer, Wayne - IIW





Subject: Re: [TN] Solder joint height










Hy Wayne,





Well, those QFNs and LCCs are deja vu all over again.  With LLCCCs we had an





obvious huge CTE-mismatch between ceramic and FR-4, with QFNs it is not so





obvious since the CTE-mismatch comes from the die--so die size and die attach





are a big part of the equation.





So it depends on the stresses developed by the thermal expansion mismatch from





the product of DNPxDCTExDT whether the thin SJs will survive long enough for





reliability.





Werner




















-----Original Message-----





From: Thayer, Wayne - IIW <[log in to unmask]<mailto:[log in to unmask]>>





To: [log in to unmask]<mailto:[log in to unmask]>





Sent: Thu, May 20, 2010 4:17 pm





Subject: [TN] Solder joint height










Should there be a spec for minimum solder joint height for leadless components?






























An old paper from Werner (mid 90's, I believe) popped up on the Internet when I






























queried this, and Werner has a statement in it that joints less than about 50






























microns thick are basically all intermetallics, but that is not necessarily a






























bad thing since the intermetallics are stronger than the solder (but more






























brittle).























































I figured since we often try to get additional height for BGA joints to improve






























reliability, we should be concerned about QFNs and LCCs.























































I grabbed a 1.5mil (37 micron) tungsten rod out of our cleanroom (used for






























clearing clogged wirebond capillaries)and started seeing if I could get that






























under my leadless components.  Couldn't get it under any of them, likewise with






























the QFNs.























































Checked Technet archives and didn't see an obvious thread, but maybe I didn't






























have the correct search parameters--if you just enter "height" you get a couple






























of thousand hits.























































Wayne Thayer























































This e-mail and any files transmitted with it may be proprietary and are






























intended solely for the use of the individual or entity to whom they are






























addressed. If you have received this e-mail in error please notify the sender.






























Please note that any views or opinions presented in this e-mail are solely those






























of the author and do not necessarily represent those of ITT Corporation. The






























recipient should check this e-mail and any attachments for the presence of






























viruses. ITT accepts no liability for any damage caused by any virus transmitted






























by this e-mail.























































______________________________________________________________________






























This email has been scanned by the MessageLabs Email Security System.






























For more information please contact helpdesk at x2960 or [log in to unmask]<mailto:[log in to unmask]><mailto:[log in to unmask]<mailto:[log in to unmask]>>






























______________________________________________________________________























































---------------------------------------------------






























Technet Mail List provided as a service by IPC using LISTSERV 15.0






























To unsubscribe, send a message to [log in to unmask]<mailto:[log in to unmask]><mailto:[log in to unmask]<mailto:[log in to unmask]>> with





following text in






























the BODY (NOT the subject field): SIGNOFF Technet






























To temporarily halt or (re-start) delivery of Technet send e-mail to






























[log in to unmask]<mailto:[log in to unmask]><mailto:[log in to unmask]<mailto:[log in to unmask]>>: SET Technet NOMAIL or (MAIL)






























To receive ONE mailing per day of all the posts: send e-mail to






























[log in to unmask]<mailto:[log in to unmask]><mailto:[log in to unmask]<mailto:[log in to unmask]>>: SET Technet Digest






























Search the archives of previous posts at: http://listserv.ipc.org/archives






























Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for






























additional information, or contact Keach Sasamori at [log in to unmask]<mailto:[log in to unmask]><mailto:[log in to unmask]<mailto:[log in to unmask]>>





or






























847-615-7100 ext.2815






























-----------------------------------------------------






























______________________________________________________________________





This email has been scanned by the MessageLabs Email Security System.





For more information please contact helpdesk at x2960 or [log in to unmask]<mailto:[log in to unmask]>





______________________________________________________________________










---------------------------------------------------





Technet Mail List provided as a service by IPC using LISTSERV 15.0





To unsubscribe, send a message to [log in to unmask]<mailto:[log in to unmask]> with following text in





the BODY (NOT the subject field): SIGNOFF Technet





To temporarily halt or (re-start) delivery of Technet send e-mail to





[log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL)





To receive ONE mailing per day of all the posts: send e-mail to





[log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest





Search the archives of previous posts at: http://listserv.ipc.org/archives





Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for





additional information, or contact Keach Sasamori at [log in to unmask]<mailto:[log in to unmask]> or





847-615-7100 ext.2815





-----------------------------------------------------





______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2