TECHNET Archives

May 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Thu, 20 May 2010 01:16:14 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Werner Engelmaier <[log in to unmask]>
Subject:
From:
Werner Engelmaier <[log in to unmask]>
Content-Type:
text/plain; charset="utf-8"
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
MIME-Version:
1.0
Parts/Attachments:
text/plain (183 lines)
 Hi Jack,
That workshop was in 2007; that is at east 2 versions of the White Paper ago. I am continuously updating the White Paper and am now shipping v.09 which is almost double in content from v.07.
Even then, there was more in the White Paper than I can put into a 3-hour workshop without overloading the audience.
Werner

 


 

 

-----Original Message-----
From: Jack Olson <[log in to unmask]>
To: [log in to unmask]
Sent: Wed, May 19, 2010 8:56 pm
Subject: Re: [TN] My first RoHS circuit board!


I took your workshop at IPC MidWest called
"How to Specify PCBs to Reliably Survive the RoHS-Mandated Lead-Free
Soldering Processes"
which was VERY informative (you are a good teacher).
but
I would like to know if there are topics or data in the White Paper that
aren't in the workshop?
surfin' the learnin' curve,
Jack

.
On Wed, May 19, 2010 at 3:29 PM, Werner Engelmaier <[log in to unmask]>wrote:

>  Hi Jack,
> Thanks for the kudos.
> Let's first be precise with our language: there is RoHS-compliant and
> RoHS-capable—not the same ting at all.
> Also, there is 'dicy'-cured, phenolic-cured as well as
> non-dicy/non-phenolic-cured; the last is designed to fix some problems with
> phenolic-cure resins.
> Unfortunately, IPC-4101, even the C revision is not adequate for
> specification purposes—that is why I developed the White Paper.
> I fully agree with Dewey's testing recommendation.
> Werner
>
>
>
>  -----Original Message-----
> From: Jack Olson <[log in to unmask]>
> To: [log in to unmask]
> Sent: Tue, May 18, 2010 5:28 pm
> Subject: [TN] My first RoHS circuit board!
>
> Well, we avoided it as long as we could, but now I have to design for RoHS
>
>
> compliance.
>
>
>
>
> I'm basically following Werner's recommendations (which don't conflict with
>
>
> anyone else's as far as I know), but I'm confused about one aspect of
>
>
> material:
>
>
> Several sources have stated that its better to use "NON-DICEY" material, but
>
>
> none of the IPC-4101 slash sheets mention dicy or non-dicy (or
>
>
> dicyandiamide).
>
>
> If we are trying /126 material, do we still have to specify non-dicy?
>
>
>
>
> thanks,
>
>
> Jack
>
>
>
>
>
>
> ______________________________________________________________________
>
>
> This email has been scanned by the MessageLabs Email Security System.
>
>
> For more information please contact helpdesk at x2960 or [log in to unmask]
>
>
> ______________________________________________________________________
>
>
>
>
> ---------------------------------------------------
>
>
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
>
>
>
> To unsubscribe, send a message to [log in to unmask] with following text in
>
>
> the BODY (NOT the subject field): SIGNOFF Technet
>
>
> To temporarily halt or (re-start) delivery of Technet send e-mail to
>
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>
>
> To receive ONE mailing per day of all the posts: send e-mail to
>
> [log in to unmask]: SET Technet Digest
>
>
> Search the archives of previous posts at: http://listserv.ipc.org/archives
>
>
>
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
>
>
> additional information, or contact Keach Sasamori at [log in to unmask] or
>
>
> 847-615-7100 ext.2815
>
>
> -----------------------------------------------------
>
>

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for 
additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------

 

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2