TECHNET Archives

May 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Werner Engelmaier <[log in to unmask]>
Date:
Wed, 19 May 2010 18:08:35 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Randall L Bock <[log in to unmask]>
Subject:
From:
Randall L Bock <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="Windows-1252"
Parts/Attachments:
text/plain (136 lines)
Werner,
Glad to sse you make a distnsion between RoHS Compliant and RoHS Capable.  There is a lot of misunderstanding regarding  definition,   

Thanks

Randy Bock Sr.


________________________________________
From: TechNet [[log in to unmask]] On Behalf Of Werner Engelmaier [[log in to unmask]]
Sent: Wednesday, May 19, 2010 4:29 PM
To: [log in to unmask]
Subject: Re: [TN] My first RoHS circuit board!

 Hi Jack,
Thanks for the kudos.
Let's first be precise with our language: there is RoHS-compliant and RoHS-capable—not the same ting at all.
Also, there is 'dicy'-cured, phenolic-cured as well as non-dicy/non-phenolic-cured; the last is designed to fix some problems with phenolic-cure resins.

 Unfortunately, IPC-4101, even the C revision is not adequate for specification purposes—that is why I developed the White Paper.
I fully agree with Dewey's testing recommendation.
Werner







-----Original Message-----
From: Jack Olson <[log in to unmask]>
To: [log in to unmask]
Sent: Tue, May 18, 2010 5:28 pm
Subject: [TN] My first RoHS circuit board!


Well, we avoided it as long as we could, but now I have to design for RoHS

compliance.



I'm basically following Werner's recommendations (which don't conflict with

anyone else's as far as I know), but I'm confused about one aspect of

material:

Several sources have stated that its better to use "NON-DICEY" material, but

none of the IPC-4101 slash sheets mention dicy or non-dicy (or

dicyandiamide).

If we are trying /126 material, do we still have to specify non-dicy?



thanks,

Jack





______________________________________________________________________

This email has been scanned by the MessageLabs Email Security System.

For more information please contact helpdesk at x2960 or [log in to unmask]

______________________________________________________________________



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to

[log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to

[log in to unmask]: SET Technet Digest

Search the archives of previous posts at: http://listserv.ipc.org/archives

Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for

additional information, or contact Keach Sasamori at [log in to unmask] or

847-615-7100 ext.2815

-----------------------------------------------------





______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2