TECHNET Archives

May 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Tue, 11 May 2010 21:31:32 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Thayer, Wayne - IIW" <[log in to unmask]>
Subject:
From:
"Thayer, Wayne - IIW" <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (103 lines)
Hi Jerry-

You are absolutely correct!  Solder mask masks solder.  Go figure!  IT IS NOT AN INSULATOR!  Been burned bad at least twice that way.

But if you remove the spheres which no longer have pads, then you likely will have no problem passing qualification (except if you remove >20% of the balls, such as 1 of 4 balls on a transistor).  When in doubt, consider underfill.

Wayne Thayer


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jerry Dengler
Sent: Tuesday, May 11, 2010 3:19 PM
To: [log in to unmask]
Subject: Re: [TN] Removing BGA Pads for Routing Clearance

Bob,

Be afraid, be very afraid.  The BGA should collapse slightly if it's
properly reflowed.  Now you will have solder balls touching the traces
with just solder mask separating it.  I know that I've read solder mask
cannot be used as a insulator, but I do not remember where.

Jerry Dengler


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Croslin, Robert
Sent: Tuesday, May 11, 2010 3:07 PM
To: [log in to unmask]
Subject: [TN] Removing BGA Pads for Routing Clearance

Dear 'Netters,

I have an engineer laying out a very small board using a .050 pitch 113
pin BGA with two rows.  He's trying to rout out from the inside row and
in order to avoid using a via, wants to delete the two adjacent pads for
routing space.  If he does, the balls that would have met with those
pads will have about a 2 mil overlay on the routed trace.  We'll be
using an LPI mask and I've told him he could risk bridging from the
solder bump should the mask crack during reflow.  He then told me our
former designer had used that trick before, but wasn't sure on which
product.  We've never had a field failure related to that condition, but
it sure made me cringe.

My question is how concerned should I be with this arrangement?


Bob Croslin
The Nielsen Company


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

This e-mail and any files transmitted with it may be proprietary and are intended solely for the use of the individual or entity to whom they are addressed. If you have received this e-mail in error please notify the sender.
Please note that any views or opinions presented in this e-mail are solely those of the author and do not necessarily represent those of ITT Corporation. The recipient should check this e-mail and any attachments for the presence of viruses. ITT accepts no liability for any damage caused by any virus transmitted by this e-mail.

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2