Hi Cedric,
Lifted external lands result form land rotation during the soldering process high temperatures—manual soldering, especially of SAC solders, being particularly bad.
They are the external; signs of possible inner-layer separation as well as barrel cracks.
Werner
-----Original Message-----
From: Cedric ORAIN <[log in to unmask]>
To: [log in to unmask]
Sent: Tue, May 11, 2010 5:22 pm
Subject: [TN] Pad lifting during manual soldering
Hello all,
We've just achieved a critical process analysis on a PCBa for high end
market. We found that the land of some of the plated through hole appeared
slightly lifted from the PCB surface.
The component was hand soldered with lead free alloy (SAC305).
Is pad lifting is acceptable? Or to what extend does it still acceptable?
I could post a picture, but I have to admit that I didn't know where or how?
Cedric ORAIN
Technical Director
www.inovelec-groupe.com
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|