Inge, it doesn't matter how they looked prior to. Being soldered. Once they melt down - the history is gone. Even though they may look like brain, they don't "have" it :-)
Vladimir
Vladimir
SENTEC Testing Laboratory Inc.
11 Canadian Road, Unit 7.
Scarborough, ON M1R 5G1
Tel: (416) 899-1882
Fax: (905) 882-8812
www.sentec.ca
-----Original Message-----
From: Inge <[log in to unmask]>
Date: Tue, 20 Apr 2010 09:36:10
To: <[log in to unmask]>
Subject: Re: [TN] SAC Shrinkage Voids in BGA Balls
High all.
Are u sure the balls are not shrinked even before soldering? I inspected
hundreds of packages before soldering and found them to be like the neck of
a Galapagos turtle. Both SAC and PbSn look all the same.
I'll send a typical picture to Steve and ask you all: do you have shrinked
balls too before action is taken?
I get question frequently from the operators, because they want see shiny
balls and not old prunes. Myself, I think the wrinkled balls has not
significance.
Inge
--------------------------------------------------
From: "Werner Engelmaier" <[log in to unmask]>
Sent: den 20 April 2010 08:55
To: <[log in to unmask]>
Subject: Re: [TN] SAC Shrinkage Voids in BGA Balls
> Hi Dave,
> A shrinkage void in an ingot occurs where it solidifies last---in its
> center.
> The same is true for SJs, except that they do not necessarily cool from
> the outside in. but a connected to various heatsinks and reservoirs---the
> component is typically a heat sink [coolest] and the PCB is a reservoir
> [hottest], with various heat transfer conditions on the surface due to
> forced air/N2.
> Overall, SJs tend to solidify first at their surface; hence, most
> shrinkage voids are to be found there.
> Werner
>
>
>
>
>
>
>
>
> -----Original Message-----
> From: David D. Hillman <[log in to unmask]>
> To: [log in to unmask]
> Sent: Tue, Apr 20, 2010 10:13 am
> Subject: Re: [TN] SAC Shrinkage Voids in BGA Balls
>
>
> Hi Bev - in theory, a shrinkage void in a solderball is the same physics
> as a shrinkage void in a aluminum or steel casting so no, the shrinkage
> void would not have to necessarily always reach a surface. However, after
> looking at several hundred SAC BGA/CSP cross-sections, I have nearly
> always (99.999%) found a path of a shrinkage void to the solderball
> surface. Because we have a very limited and very small molten solder
> "volume", I think you will find a surface connection. And I guess I'll
> bite - why the question?
>
> Dave Hillman
> Rockwell Collins
> [log in to unmask]
>
>
>
>
> Bev Christian <[log in to unmask]>
> Sent by: TechNet <[log in to unmask]>
> 04/20/2010 08:16 AM
> Please respond to
> TechNet E-Mail Forum <[log in to unmask]>; Please respond to
> Bev Christian <[log in to unmask]>
>
>
> To
> [log in to unmask]
> cc
>
> Subject
> [TN] SAC Shrinkage Voids in BGA Balls
>
>
>
>
>
>
> TechNetters,
> Do all SAC shrinkage voids in BGA balls reach/start at the surface of
> the ball? I realize I may be stumped by a 2D cross-section of a 3D
> phenomenon, but I thought I would ask this august body.
> Bev
> RIM
>
> ---------------------------------------------------------------------
> This transmission (including any attachments) may contain confidential
> information, privileged material (including material protected by the
> solicitor-client or other applicable privileges), or constitute non-public
> information. Any use of this information by anyone other than the intended
> recipient is prohibited. If you have received this transmission in error,
> please immediately reply to the sender and delete this information from
> your system. Use, dissemination, distribution, or reproduction of this
> transmission by unintended recipients is not authorized and may be
> unlawful.
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
>
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for
> additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
>
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|