Aqualine 6000 is halide-free, ORH0. Must be washed, washable in hot DI
water.
Karen Tellefsen - Electrical Testing
[log in to unmask]
908-791-3069
"Guy M. Ramsey"
<gramsey@RDCIRCUI
TS.COM> To
Sent by: TechNet [log in to unmask]
<[log in to unmask]> cc
Subject
04/19/2010 02:42 Re: [TN] Flux-Cored Wire Solder:
PM Halide / Halide-Free
Please respond to
TechNet E-Mail
Forum
<[log in to unmask]>
; Please respond
to
"Guy M. Ramsey"
<gramsey@RDCIRCUI
TS.COM>
Amtech makes a wire core solder with Halide free watersoluble flux. You
should
clean it but it cleans fairly easily. If you are looking to change your
cleaning
process, I recommend you look at it. We clean it with a spot steam cleaner.
If you are staying with alcohol you cannot use it.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------