TECHNET Archives

April 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Jack Olson <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Jack Olson <[log in to unmask]>
Date:
Wed, 14 Apr 2010 17:43:36 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (121 lines)
Well, now you are showing off!

I believe the modern "impurity" is a .2% cobalt to add hardness,

so I guess my questions for curiosity should have been
"did standard knoop hardness change over the years?"
and
"has gold thickness been gradually reduced over the years?"
but my REAL question is:
"Has anyone experienced switch contact failures using the IPC
recommended 150 knoop, 118uin. Nickel min, 31.5uin. Gold min.?"
thanks,
jack

On Wed, Apr 14, 2010 at 5:19 PM, Inge <[log in to unmask]> wrote:

> Jack,
> like you say, it's more to it....gold thickness is not the one and only
> parameter.  Other factors are contact asperity, contact geometry, contact
> area vs. current, wipe pressure, switch slide coefficient, underlying
> plating, life expectancy and at least half a dozen more parameters. I was
> specialist on electromechanical and manual switches decades ago, don't
> remember all details, but I can tell you this: if you count on gold
> thickness only, you don't know what you are shipping.  93.7% Au? We did not
> name that Gold at all. We talked about maximum 0.1% impurities.  The more
> impurities, the higher the friction coefficient. Well, I don't know what
> level of quality you speak for. I was in the HiRel, so maybe I'm too
> demanding. Anyway,  My advice (which you will probably frown at) is
> basic metal ?? your wiper
> 300 uinches of pure Nickel
> 25 uinches of Rhodium over Nickel
> 5 uinches of soft gold (gold works as 'lubricant')
>
> The above based on a qualified switch mechanism.  If that is not the case,
> not even 160 uinches of gold  will work for a very long life.  160 uinches!
> Never heard of such a lot of gold. When extrem current switching is actual,
> one use to work with mercury switches, microswitches or like.
>
> Don't listen to me, I'm from an era when we dismantled switches and relays
> and measured all contact parameters and stored the  test data for minimum 10
> years. And all our own test equipments were sent to a qualfied reference
> lab. Madness?
>
> Inge
>
> --------------------------------------------------
> From: "Jack Olson" <[log in to unmask]>
> Sent: den 14 April 2010 14:14
> To: <[log in to unmask]>
> Subject: [TN] Question for "Old-Timers" about Gold
>
>   ya know, every time I think I know enough about a particular subject,
>> something comes along to make me realize there is more to it....
>>
>> I need to order some boards using a fabrication drawing that hasn't been
>> updated in over fifteen years.
>> We need Hard Gold Electroplating for a rotary switch contacts.
>> One of the notes calls for gold knoop hardness 200-300, thickness 130-230
>> uin. 93.7% purity
>> The last FAI report showed gold thickness of 160 uin. All other historical
>> records are lost in the shifting sands of time
>>
>> Our vendor has knoop hardness 150, 99.7% purity and says gold requirement
>> is
>> too thick.
>>
>> IPC says knoop 150, gold minimum 31.5 uin. for edge connector fingers,
>> which
>> I assume is the same for contacts (doesn't seem to be addressed)
>>
>> Printed Circuits Handbook says knoop 150,  thickness 25-50 uin for
>> non-military, 99.8% gold purity
>>
>> Has gold plating changed that much since then?
>> Is there a danger of wear-out if I get 50uin. gold plating when our old
>> boards were 160 uin.?
>>
>> surfin' the learnin' curve,
>> Jack
>>
>>
>> ______________________________________________________________________
>> This email has been scanned by the MessageLabs Email Security System.
>> For more information please contact helpdesk at x2960 or [log in to unmask]
>> ______________________________________________________________________
>>
>> ---------------------------------------------------
>> Technet Mail List provided as a service by IPC using LISTSERV 15.0
>> To unsubscribe, send a message to [log in to unmask] with following text in
>> the BODY (NOT the subject field): SIGNOFF Technet
>> To temporarily halt or (re-start) delivery of Technet send e-mail to
>> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>> To receive ONE mailing per day of all the posts: send e-mail to
>> [log in to unmask]: SET Technet Digest
>> Search the archives of previous posts at:
>> http://listserv.ipc.org/archives
>> Please visit IPC web site
>> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
>> information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
>> ext.2815
>> -----------------------------------------------------
>>
>
>


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2