We pot a lot of product. It is common practice to de-pot units for
analysis. It is not difficult. A little heat and an orange stick will
remove most.
I once worked on a contract to build secure terminals that had a wire loop
suspended in the potting that would erase the program if broken - maybe
better than nothing ,you would have to give me two of those to safely
de-pot it for you.
Potting would stop the curious, but not the really curious.
Also be careful of choosing something too hard to discourage removal, high
CTE mismatch between potting and board will cause failures during thermal
cycle. If it is a new process to you, make sure you qualify it.
Roger Mack P.Eng.
Manufacturing Specialist
Parker Hannifin Electronic Controls
Electronic Controls Division
1305 Clarence Avenue
Winnipeg, MB R3T 1T4 Canada
direct 204 453 3339 x373
[log in to unmask]
www.parker.com/ecd
Ioan Tempea <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
04-07-2010 13:54
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Ioan Tempea <[log in to unmask]>
To
[log in to unmask]
cc
Subject
[TN] Reverse engineering proofing
Dear Technos,
We want to prevent reverse engineering of a few products that we assemble,
as much as we can. What are the proofing methods you use?
An idea that came up was to cover the surface of the cards with potting.
If this makes sense, what substance to use?
Thanks,
Ioan Tempea, ing.
Ingénieur Principal de Fabrication / Senior Manufacturing Engineer
T | 450.967.7100 ext.244
E | [log in to unmask] <mailto:[log in to unmask]>
W | www.digico.cc <http://www.digico.cc/>
N'imprimer que si nécessaire - Print only if you must
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
PLEASE NOTE: The preceding information may be confidential or
privileged. It only should be used or disseminated for the purpose
of conducting business with Parker. If you are not an intended
recipient, please notify the sender by replying to this message and
then delete the information from your system. Thank you for your
cooperation.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|