I am happy to give people 40 year guarantees, but that is because I am soon
to retire. :)
More usefully http://www.metallurgy.nist.gov/solder/ is probably a good
resource to click in from.
Regards
Mike
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Inge
Sent: Wednesday, April 14, 2010 7:14 PM
To: [log in to unmask]
Subject: Re: [TN] solder creep charts
Talking creepy things, has anyone of you performed practical tests to
confirm theoretical calculations on life of BGA boards? We sell products
with life expectancy like 20 years minimum. Theory is one thing, but what
will really happen after five years, ten years, fifteen year...? Allright,
so many design variants, so many factors and difficulties to jugdge the
result. If I put the question this way: do any of you fear that your BGA
board will be failure reported long before the guaranteed TTF? ......Ja.
ja, I know. Noone will let the whole world know. My question suits better
in the waste bin. We have done ver 100,000 tempcycles on BGA boards, and I
hoped that someone (mad) had done same.
/Inge
--------------------------------------------------
From: "Roger Mack" <[log in to unmask]>
Sent: den 14 April 2010 07:23
To: <[log in to unmask]>
Subject: [TN] solder creep charts
> Does anyone have a detailed solder creep graph (shear stress N/mm˛ vs.
> time to rupture) for tin lead solder?
> I have been using Figure 4.35 from Klein Wassink's Soldering in
> Electronics. This graph starts at a shear stress of 1.
> We have run a ProE computer model that shows a shear stress value of
> 0.6N/mm˛ on the connector pins of two boards that are mounted together. We
> have placed some samples to bake at the maximum service condition
> temperature to validate the computer model is realistic. It does not take
> much of an extrapolation error on a small text book graph to be off by an
> order of magnitude.
>
>
>
> Roger Mack P.Eng.
> Manufacturing Specialist
> Parker Hannifin Electronic Controls
> Electronic Controls Division
> 1305 Clarence Avenue
> Winnipeg, MB R3T 1T4 Canada
> direct 204 453 3339 x373
> [log in to unmask]
> www.parker.com/ecd
>
>
>
>
>
> PLEASE NOTE: The preceding information may be confidential or
> privileged. It only should be used or disseminated for the purpose
> of conducting business with Parker. If you are not an intended
> recipient, please notify the sender by replying to this message and
> then delete the information from your system. Thank you for your
> cooperation.
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
***This email, its content, and any files transmitted with it, are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient, please contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination, or other use of, or taking of any action in reliance upon this information by persons or entities other than the intended recipient is prohibited.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|