This subject brings up an interesting story about the invention of electroplating.
Seems that before electroplating, gold was "plated" on to metals by dissolving it in Mercury, and wiped on to the part to be plated. The part was then baked to evaporate the Mercury...
Clearly, OSHA was not yet even a glint in the government's eye....
This method was causing all the "platers" to die off rapidly. So, somebody developed gold plating, to minimize the death rate of the platers!
Rudy Sedlak
RD Chemical Company
--- On Thu, 4/29/10, Cedric ORAIN <[log in to unmask]> wrote:
From: Cedric ORAIN <[log in to unmask]>
Subject: [TN] Gilded PCB
To: [log in to unmask]
Date: Thursday, April 29, 2010, 8:04 AM
Hello all,
I've just heard about "Gilded PCB" for the first time. What exactly "Gilded"
stands for? Just a common ENIG finition? Or something more precise?
Thank you for your help.
Cedric
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|