Amtech makes a wire core solder with Halide free watersoluble flux. You should
clean it but it cleans fairly easily. If you are looking to change your cleaning
process, I recommend you look at it. We clean it with a spot steam cleaner.
If you are staying with alcohol you cannot use it.
---------------------------------------------------