Hi Victor,
IPC has just updated J-STD-001 to Rev E.
In RevE, the temperature and humidity in a factory are recommended as following:
For operator comfort and solderability maintenance, the temperature should be maintained between 18°C [64.4°F] and 30°C [86°F] and the relative humidity should not exceed 70%. For process control, more restrictive temperature and humidity limits may be required.
In order to control the factory environment, I think you should buy J-STD-001E. It's not free.
If you need to buy any IPC documents, please contact me.
Hao Yu 郝 宇
IPC
Mobile: 13823187909
________________________________
发件人: TGAsia [[log in to unmask]] 代表 victor [[log in to unmask]]
发送时间: 2010年4月27日 23:51
收件人: Listserv TGAsia
主题: Re: [TGAsia] 答复: [TG Asia] SMT车 间环境温湿度的 要求
Dear Snow,
Could you please share the original text with us? So we can convince our customer.
Thanks with best regards,
Victor
在2010-04-27 14:03:02,snow_fu <[log in to unmask]> 写道:
Please refer to IPC J-STD-001 4.2.2.
Temperature control spec is 18ºC ~ 30ºC & Humidity is 30% ~ 70%.
Actually We need to control humidity not high than 60% since there are some MSD component using in factory.
发件人: TGAsia [mailto:[log in to unmask]<mailto:[log in to unmask]>] 代表 txb1027
发送时间: 2010年4月26日 20:10
收件人: [log in to unmask]<mailto:[log in to unmask]>
主题: [TGAsia] SMT车间环境温湿度的要求
Dear all,
请教一个SMT车间温湿度的控制要求,引用IPC什么标准?当前我们是18-26.度湿度是40%-60%,总是不达标,想修改这个范围,但不知道引用什么标准。
________________________________
有域名马上来,网易免费送你200户域名邮箱<http://ym.163.com/?from=od1>
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]<mailto:[log in to unmask]>
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]<mailto:[log in to unmask]>
______________________________________________________________________
________________________________
有域名马上来,网易免费送你200户自主域名邮箱<http://ym.163.com/?from=od1>
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|