As others have said there is insufficient data here Pradeep, you need to
describe the issue fully. I.e. are the boards delaminating in specific areas
such as a BGA via hole field? Size/description of the d-laminations, is it
the top or back of the board etc - photo's would also help.
Regards
John Burke
(408) 515 4992
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Pradeep Menon
Sent: Thursday, April 01, 2010 11:11 PM
To: [log in to unmask]
Subject: [TN] Outer layer separation
Importance: High
Dear all,
Wanted some inputs on a problem which we are facing currently
We observe a separation, rather tendency for separation, on 2.5mm thick MLB
boards when subjected to 3X 288 deg 10 sec thermal stress. This is mostly
found only on one side ie in one of the outerlayers, and very few on both
outer layers. The inner layers are intact.
We use N4000-6 as well as 4000-13EP laminates for fabricating PCBs and we
use laminate construction for the stack up. We do Plasma desmear followed by
a run thru permanganate too. We tried various parameters in drilling as well
as reviewed all the basic electroless / electroplating parameters , and all
were found as desired.
We use 1-1.2 microns thick electroless copper followed by a flash
electrolplated copper of about 12 microns before pattern printing. The board
is then pattern plated to achieve a minimum PTH copper of 30 microns.
Looking forward fro ur inputs
Rgds
Pradeep
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|