Have you tried Electro-form or Slick and Ultra-Slick material for your stencil material.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Cedric ORAIN
Sent: Wednesday, April 21, 2010 3:12 PM
To: [log in to unmask]
Subject: Re: [TN] R: [TN] Head in Pillow and grapping effects mitigation without Nitrogen
We still using type 4 that give good results with 110um (laser cut nickel
stencil).
-----Message d'origine-----
De : TechNet [mailto:[log in to unmask]] De la part de Gabriele Sala
Envoyé : mercredi 21 avril 2010 22:04
À : [log in to unmask]
Objet : [TN] R: [TN] Head in Pillow and grapping effects mitigation without
Nitrogen
Hi Cedric,
What are you using as powder size in your actual solder paste ? :
- Type-4 ?
- Type-5 ?
For your application Type-4 could work, better if Type-5, but as you know as
powder size gets smaller the risk of powder oxidation increases, so N2 could
be a must during reflow.
Gabriele
-----Messaggio originale-----
Da: TechNet [mailto:[log in to unmask]] Per conto di Cedric ORAIN
Inviato: mercoledì 21 aprile 2010 21.55
A: [log in to unmask]
Oggetto: Re: [TN] Head in Pillow and grapping effects mitigation without
Nitrogen
I wasn't thinking about warpage as HOP cause, I will take care of that
:thanks.
And no, I've never encountered grapping and HOP at the same time. The point
is that it deals with 2 kinds of defects that are coming with
miniaturization.
-----Message d'origine-----
De : TechNet [mailto:[log in to unmask]] De la part de Genny Gibbard
Envoyé : mercredi 21 avril 2010 21:30
À : [log in to unmask]
Objet : Re: [TN] Head in Pillow and grapping effects mitigation without
Nitrogen
At Apex, one of the primary causes reported for HOP was component
warping.
However, if you are also getting graping at the same time, then to me it
appears that it is a solder quality/heat issue.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier
Sent: April 21, 2010 1:05 PM
To: [log in to unmask]
Subject: Re: [TN] Head in Pillow and grapping effects mitigation without
Nitrogen
Hi Cedric,
What do you mean by 'grapping effect"?
You do not say where you find 'Head-on-Pillow' defects-they can occur at
the BGA periphery and in the BGA center and the root cause is quite
different.
HOP at the periphery is a solderability issue and certainly involves the
choice of paste/flux.
HOP in the BGA center means you do not have enough heat there to get the
solder ball to a low-viscosity liquid state-that means you need to
increase the peak reflow temperature.
One of the reasons for larger solder volumes is to achieve greater SJ
stand-off heights to improve reliability.
Werner
-----Original Message-----
From: Cedric ORAIN <[log in to unmask]>
To: [log in to unmask]
Sent: Wed, Apr 21, 2010 2:38 pm
Subject: [TN] Head in Pillow and grapping effects mitigation without
Nitrogen
Hello all,
Very fine pitch BGAs (typically 0.5mm) and 0201 chips are becoming
common in our company for some months.
We recently have to face with new defects type such as grapping effect
and head in pillow defect.
The solder paste we use has been qualified for even smaller component
(WLP, 0.4mm pitch) but in Nitrogen atmosphere.
I'm now wondering if this solder paste is suitable with Air reflow. I'm
also wondering if a solder paste suitable in that case even exists.
Having a look to this study from intel (link hereunder, page 31), I
found that the people from Intel are recommending a solder paste volume
larger than 2000 mil^3 as a minimum.
http://edc.intel.com/Download.aspx?id=3044&returnurl=/default.aspx
That is, off-course, impossible for a VFBGA (which solder paste deposit
is closer to 900mil^3) but this reading makes me feel uncomfortable.
So the question is: is it possible to find out a solder paste which is
suitable for VFBGA assembly in Air reflow?
If it is not against TechNet rules, have you some solder paste
references that you could advise?
Here are some additional details: ENIG PCB finition, SAC305 Alloy.
Cedric ORAIN
Technical Director
Electronic Manufacturing Services
www.inovelec-groupe.com
PS: I'm very new and I'm also French. I wish it will not be too much for
you! Anyway, thank for being patient if I have difficulties to
understand.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
No virus found in this incoming message.
Checked by AVG - www.avg.com
Version: 8.5.437 / Virus Database: 271.1.1/2826 - Release Date: 04/21/10
11:09:00
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|