TECHNET Archives

April 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Glidden, Kevin" <[log in to unmask]>
Date:
Mon, 19 Apr 2010 11:34:17 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Paul Edwards <[log in to unmask]>
Subject:
From:
Paul Edwards <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (132 lines)
Ken,

What halide-free spec are you using?

Non-semiconductor grade alcohol can have halides as well as the water source for your DI...


Paul

Paul Edwards
Surface Art Engineering


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Glidden, Kevin
Sent: Monday, April 19, 2010 8:42 AM
To: [log in to unmask]
Subject: Re: [TN] Flux-Cored Wire Solder: Halide / Halide-Free

Great question, Joe.

We use a water soluble paste, followed by DI water wash.

Secondary hand soldering uses RMA flux and (sigh) the fabled isopropyl alcohol localized hand cleaning.  I'm also working on improving this and moving to a saponified wash for all levels of soldering....

But, for now, (and part of the basis of my concern) the hand soldering with the wire is only hand cleaned, thus my desire to take use halide-free and hopefully make it less risky...


Kevin Glidden
Manufacturing Engineer
Astronics Luminescent Systems Inc.

-----Original Message-----
From: Kane, Joseph E (US SSA) [mailto:[log in to unmask]] 
Sent: Monday, April 19, 2010 11:33 AM
To: [log in to unmask]
Subject: Re: [TN] Flux-Cored Wire Solder: Halide / Halide-Free

Kevin:

Are you cleaning off the flux residues?  If this is a no-clean 
process, and you're leaving residues on, then interactions between 
the chemistries become more important.

-Joe 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Glidden, Kevin
Sent: Monday, April 19, 2010 11:18 AM
To: [log in to unmask]
Subject: [TN] Flux-Cored Wire Solder: Halide / Halide-Free

Greetings,

I've recently been looking into changing out some solder materials.  I was forced to change solder pastes due to product obsolescence.  I am now in the process of verifying compatibility of the hand soldering fluxes and solders with the new paste.  My current paste is halide-free.  My current flux cored wire solder is not.  I asked a supplier about halide-free flux-cored wire solder and the basic response is that you can get it, but it's really non-standard, so it's a lot more expensive with larger min-buys.  Indeed, after I looked at a few websites about product offerings, it appears most flux-cored wire solders are not halide-free.  I understand that I can basically use any materials I like as long as I test it out and can prove my "recipe" is safe to the overall product reliability, but seemingly halide-free is a safer way to in general.

So I am wondering:

1) Am I worrying about nothing (matching halide-free paste with halide free solder wires)?

2) Is it really not all that common to use halide-free flux-cored wire solders?

As always, thank you in advance...

Kevin Glidden

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------


==============================================================================

This email and any attachments thereto may contain private, confidential, and
privileged material for the sole use of the intended recipient. Any review, copying,
or distribution of this email (or any attachments thereto) by others is strictly prohibited.
If you are not the intended recipient, please contact [log in to unmask]
immediately and permanently delete the original and any copies of this email and
any attachments thereto. 

==============================================================================


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2